Structure of magnetron hydroxyapatite films with small stoichiometry deviation
Phase composition, coherence lengths and micro-strain level in hydroxyapatite films with controlled deviation from stoichiometry (Ca/P = 1.67) were measured by methods of X-ray diffraction and X-ray fluorescent analysis. It was established that at Ca/P = 1.6±0.03, hydroxyapatite layers with thicknes...
Збережено в:
Дата: | 2016 |
---|---|
Автори: | , , |
Формат: | Стаття |
Мова: | English |
Опубліковано: |
НТК «Інститут монокристалів» НАН України
2016
|
Назва видання: | Functional Materials |
Теми: | |
Онлайн доступ: | http://dspace.nbuv.gov.ua/handle/123456789/121404 |
Теги: |
Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
|
Назва журналу: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
Цитувати: | Structure of magnetron hydroxyapatite films with small stoichiometry deviation / I.F. Mikhailov, V.V. Starikov, A.A. Baturin // Functional Materials. — 2016. — Т. 23, № 3. — С. 394-397. — Бібліогр.: 8 назв. — англ. |
Репозитарії
Digital Library of Periodicals of National Academy of Sciences of Ukraineid |
irk-123456789-121404 |
---|---|
record_format |
dspace |
spelling |
irk-123456789-1214042017-06-15T03:02:34Z Structure of magnetron hydroxyapatite films with small stoichiometry deviation Mikhailov, I.F. Starikov, V.V. Baturin, A.A. Characterization and properties Phase composition, coherence lengths and micro-strain level in hydroxyapatite films with controlled deviation from stoichiometry (Ca/P = 1.67) were measured by methods of X-ray diffraction and X-ray fluorescent analysis. It was established that at Ca/P = 1.6±0.03, hydroxyapatite layers with thickness 2m on the niobium substrates were practically single-phase but differed by the coherence lengths and micro-strain levels for different crystallographic directions: the coherence length along [001] was commensurable with the film thickness and much exceeded the values for [101] and [111] directions. The micro-strain level ε for [001] direction reached (1.3÷1.7)·10⁻³ being by an order higher than for [101] and [111] directions. That testifies constrained growth conditions along [001] with the high homogeneity of the lattice period of the hydroxyapatite film. 2016 Article Structure of magnetron hydroxyapatite films with small stoichiometry deviation / I.F. Mikhailov, V.V. Starikov, A.A. Baturin // Functional Materials. — 2016. — Т. 23, № 3. — С. 394-397. — Бібліогр.: 8 назв. — англ. DOI: dx.doi.org/10.15407/fm23.03.394 1027-5495 http://dspace.nbuv.gov.ua/handle/123456789/121404 en Functional Materials НТК «Інститут монокристалів» НАН України |
institution |
Digital Library of Periodicals of National Academy of Sciences of Ukraine |
collection |
DSpace DC |
language |
English |
topic |
Characterization and properties Characterization and properties |
spellingShingle |
Characterization and properties Characterization and properties Mikhailov, I.F. Starikov, V.V. Baturin, A.A. Structure of magnetron hydroxyapatite films with small stoichiometry deviation Functional Materials |
description |
Phase composition, coherence lengths and micro-strain level in hydroxyapatite films with controlled deviation from stoichiometry (Ca/P = 1.67) were measured by methods of X-ray diffraction and X-ray fluorescent analysis. It was established that at Ca/P = 1.6±0.03, hydroxyapatite layers with thickness 2m on the niobium substrates were practically single-phase but differed by the coherence lengths and micro-strain levels for different crystallographic directions: the coherence length along [001] was commensurable with the film thickness and much exceeded the values for [101] and [111] directions. The micro-strain level ε for [001] direction reached (1.3÷1.7)·10⁻³ being by an order higher than for [101] and [111] directions. That testifies constrained growth conditions along [001] with the high homogeneity of the lattice period of the hydroxyapatite film. |
format |
Article |
author |
Mikhailov, I.F. Starikov, V.V. Baturin, A.A. |
author_facet |
Mikhailov, I.F. Starikov, V.V. Baturin, A.A. |
author_sort |
Mikhailov, I.F. |
title |
Structure of magnetron hydroxyapatite films with small stoichiometry deviation |
title_short |
Structure of magnetron hydroxyapatite films with small stoichiometry deviation |
title_full |
Structure of magnetron hydroxyapatite films with small stoichiometry deviation |
title_fullStr |
Structure of magnetron hydroxyapatite films with small stoichiometry deviation |
title_full_unstemmed |
Structure of magnetron hydroxyapatite films with small stoichiometry deviation |
title_sort |
structure of magnetron hydroxyapatite films with small stoichiometry deviation |
publisher |
НТК «Інститут монокристалів» НАН України |
publishDate |
2016 |
topic_facet |
Characterization and properties |
url |
http://dspace.nbuv.gov.ua/handle/123456789/121404 |
citation_txt |
Structure of magnetron hydroxyapatite films with small stoichiometry deviation / I.F. Mikhailov, V.V. Starikov, A.A. Baturin // Functional Materials. — 2016. — Т. 23, № 3. — С. 394-397. — Бібліогр.: 8 назв. — англ. |
series |
Functional Materials |
work_keys_str_mv |
AT mikhailovif structureofmagnetronhydroxyapatitefilmswithsmallstoichiometrydeviation AT starikovvv structureofmagnetronhydroxyapatitefilmswithsmallstoichiometrydeviation AT baturinaa structureofmagnetronhydroxyapatitefilmswithsmallstoichiometrydeviation |
first_indexed |
2023-10-18T20:39:22Z |
last_indexed |
2023-10-18T20:39:22Z |
_version_ |
1796150768802201600 |