Scintillation properties of Eu²⁺-doped SrCl₂ and CsSrCl₃ single crystals
Eu²⁺-doped CsSrCl₃ scintillation crystals with activator concentration 0.5, 1 and 5 mol. % and SrCl₂: Eu²⁺ material doped with 1 mol. % of the activator have been grown by Bridg-man-Stockbarger method. The radioluminescence spectra of CsSrCl₃: Eu²⁺ materials include a narrow band with the maximum wh...
Збережено в:
Дата: | 2012 |
---|---|
Автори: | , , , , , , , , , |
Формат: | Стаття |
Мова: | English |
Опубліковано: |
НТК «Інститут монокристалів» НАН України
2012
|
Назва видання: | Functional Materials |
Теми: | |
Онлайн доступ: | http://dspace.nbuv.gov.ua/handle/123456789/135294 |
Теги: |
Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
|
Назва журналу: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
Цитувати: | Scintillation properties of Eu²⁺-doped SrCl₂ and CsSrCl₃ single crystals/ V.L. Cherginets, A.Yu. Grippa, T.P. Rebrova, Yu.N. Datsko, T.V. Ponomarenko, N.V. Rebrova, N.N. Kosinov, O.A. Tarasenko, Yu.I. Dolzhenko, O.V. Zelenskaya // Functional Materials. — 2012. — Т. 19, № 2. — С. 187-191. — Бібліогр.: 7 назв. — англ. |
Репозитарії
Digital Library of Periodicals of National Academy of Sciences of UkraineРезюме: | Eu²⁺-doped CsSrCl₃ scintillation crystals with activator concentration 0.5, 1 and 5 mol. % and SrCl₂: Eu²⁺ material doped with 1 mol. % of the activator have been grown by Bridg-man-Stockbarger method. The radioluminescence spectra of CsSrCl₃: Eu²⁺ materials include a narrow band with the maximum which position is shifted from 437 to 448 nm with Eu²⁺ concentration increase and the spectrum for SrCl₂:Eu²⁺ contains a band with the maximum at 414 nm. The light yield of CsSrCl₃:Eu²⁺ material achieves maximal value at 5 mol. % of Eu²⁺ and it is equal to 39 % in respect to Nal:TI (ca 16,000 photons per MeV) and energetic resolution R is 11.5 %, whereas for SrCl₂:l mol. % of Eu²⁺ the light yield consists 30 % (ca 12,000 photons per MeV) and R = 9.2 %. The scintillation pulse decay curves for CsSrCl₃:Eu²⁺ is described by two components with the decay constants 420 ns and 2.8 ps and the fraction of the faster component is 0.3. |
---|