Physico-mechanical and physicochemical interaction at sintering of cBN-TiB₂ composites under ultrahigh pressure

It has been shown in experiment that at the reactive sintering of cubic boron nitride with aluminum under high pressures and temperatures, addition of TiB₂ results in shifting of the reaction towards crystallization of aluminum diboride instead of higher diborides and provides the absence of residua...

Full description

Saved in:
Bibliographic Details
Main Authors: Garbuz, T.O., Bezhenar, M.P., Bozhko, S.A., Bilyavina, N.M.
Format: Article
Language:English
Published: НТК «Інститут монокристалів» НАН України 2007
Series:Functional Materials
Online Access:http://dspace.nbuv.gov.ua/handle/123456789/136424
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:It has been shown in experiment that at the reactive sintering of cubic boron nitride with aluminum under high pressures and temperatures, addition of TiB₂ results in shifting of the reaction towards crystallization of aluminum diboride instead of higher diborides and provides the absence of residual aluminum in the reaction products. The calculated values of residual thermal stresses in cBN and TiB₂ phases sintered under 8GPa at 2300 K are considerably lower than the phase flexural strength.