Internal structure parameters and synthesis conditions of polycrystalline diamond films
The dependence of the internal structure parameters of polycrystalline diamond films on their thickness that is a function of the synthesis duration at the specified temperature has been studied. It has been established that the block size and the film micro-distortions are reduced at the temperatur...
Збережено в:
Дата: | 2007 |
---|---|
Автори: | , , |
Формат: | Стаття |
Мова: | English |
Опубліковано: |
НТК «Інститут монокристалів» НАН України
2007
|
Назва видання: | Functional Materials |
Онлайн доступ: | http://dspace.nbuv.gov.ua/handle/123456789/136502 |
Теги: |
Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
|
Назва журналу: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
Цитувати: | Internal structure parameters and synthesis conditions of polycrystalline diamond films / S.N. Samsonenko, N.D. Samsonenko, Z.I. Kolupaeva // Functional Materials. — 2007. — Т. 14, № 2. — С. 212-217. — Бібліогр.: 12 назв. — англ. |
Репозитарії
Digital Library of Periodicals of National Academy of Sciences of Ukraineid |
irk-123456789-136502 |
---|---|
record_format |
dspace |
spelling |
irk-123456789-1365022018-06-17T03:09:16Z Internal structure parameters and synthesis conditions of polycrystalline diamond films Samsonenko, S.N. Samsonenko, N.D. Kolupaeva, Z.I. The dependence of the internal structure parameters of polycrystalline diamond films on their thickness that is a function of the synthesis duration at the specified temperature has been studied. It has been established that the block size and the film micro-distortions are reduced at the temperature 1073 K and the gas mixture pressures of 10.6 and 21.3 kPa. The dislocation density remains almost unchanged when passing from "thin" films (4-6 μm) to "thick" ones (10-12 μm). At the temperature 1173 K and gas mixture pressures 10.6 and 21.3 kPa, the block size diminishes and micro-distortions increase when the film thickness rises. The dislocation density increases in this case. These two polycrystalline diamond films synthesis regimes are of good prospects for study of the polycrystalline diamond films electron properties formation, since the dislocations give rise to electrical active centers in diamond materials. The recrystallization of the polycrystalline diamond films crystallites starts at 1273 K and pressures of 10.6, 21.3, 31.9 kPa or at pressure 31.9 kPa and synthesis temperatures 1073 K, 1173 K, 1273 K. That effect hinders the control dislocation density control. 2007 Article Internal structure parameters and synthesis conditions of polycrystalline diamond films / S.N. Samsonenko, N.D. Samsonenko, Z.I. Kolupaeva // Functional Materials. — 2007. — Т. 14, № 2. — С. 212-217. — Бібліогр.: 12 назв. — англ. 1027-5495 http://dspace.nbuv.gov.ua/handle/123456789/136502 en Functional Materials НТК «Інститут монокристалів» НАН України |
institution |
Digital Library of Periodicals of National Academy of Sciences of Ukraine |
collection |
DSpace DC |
language |
English |
description |
The dependence of the internal structure parameters of polycrystalline diamond films on their thickness that is a function of the synthesis duration at the specified temperature has been studied. It has been established that the block size and the film micro-distortions are reduced at the temperature 1073 K and the gas mixture pressures of 10.6 and 21.3 kPa. The dislocation density remains almost unchanged when passing from "thin" films (4-6 μm) to "thick" ones (10-12 μm). At the temperature 1173 K and gas mixture pressures 10.6 and 21.3 kPa, the block size diminishes and micro-distortions increase when the film thickness rises. The dislocation density increases in this case. These two polycrystalline diamond films synthesis regimes are of good prospects for study of the polycrystalline diamond films electron properties formation, since the dislocations give rise to electrical active centers in diamond materials. The recrystallization of the polycrystalline diamond films crystallites starts at 1273 K and pressures of 10.6, 21.3, 31.9 kPa or at pressure 31.9 kPa and synthesis temperatures 1073 K, 1173 K, 1273 K. That effect hinders the control dislocation density control. |
format |
Article |
author |
Samsonenko, S.N. Samsonenko, N.D. Kolupaeva, Z.I. |
spellingShingle |
Samsonenko, S.N. Samsonenko, N.D. Kolupaeva, Z.I. Internal structure parameters and synthesis conditions of polycrystalline diamond films Functional Materials |
author_facet |
Samsonenko, S.N. Samsonenko, N.D. Kolupaeva, Z.I. |
author_sort |
Samsonenko, S.N. |
title |
Internal structure parameters and synthesis conditions of polycrystalline diamond films |
title_short |
Internal structure parameters and synthesis conditions of polycrystalline diamond films |
title_full |
Internal structure parameters and synthesis conditions of polycrystalline diamond films |
title_fullStr |
Internal structure parameters and synthesis conditions of polycrystalline diamond films |
title_full_unstemmed |
Internal structure parameters and synthesis conditions of polycrystalline diamond films |
title_sort |
internal structure parameters and synthesis conditions of polycrystalline diamond films |
publisher |
НТК «Інститут монокристалів» НАН України |
publishDate |
2007 |
url |
http://dspace.nbuv.gov.ua/handle/123456789/136502 |
citation_txt |
Internal structure parameters and synthesis conditions of polycrystalline diamond films / S.N. Samsonenko, N.D. Samsonenko, Z.I. Kolupaeva // Functional Materials. — 2007. — Т. 14, № 2. — С. 212-217. — Бібліогр.: 12 назв. — англ. |
series |
Functional Materials |
work_keys_str_mv |
AT samsonenkosn internalstructureparametersandsynthesisconditionsofpolycrystallinediamondfilms AT samsonenkond internalstructureparametersandsynthesisconditionsofpolycrystallinediamondfilms AT kolupaevazi internalstructureparametersandsynthesisconditionsofpolycrystallinediamondfilms |
first_indexed |
2023-10-18T21:13:18Z |
last_indexed |
2023-10-18T21:13:18Z |
_version_ |
1796152239357689856 |