cBN based materials with TiN-Al binder phase: sintering, structure, properties
Cubic boron nitride material was produced via high pressure and high temperature sintering with titanium nitride and aluminum as binder phase. Microstructure, phase composition and physical-mechanical properties of the material were subject of current research. Formation of TiB₂ and AlN was establis...
Saved in:
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Інститут надтвердих матеріалів ім. В.М. Бакуля НАН України
2019
|
Series: | Породоразрушающий и металлообрабатывающий инструмент – техника и технология его изготовления и применения |
Subjects: | |
Online Access: | http://dspace.nbuv.gov.ua/handle/123456789/159970 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Cubic boron nitride material was produced via high pressure and high temperature sintering with titanium nitride and aluminum as binder phase. Microstructure, phase composition and physical-mechanical properties of the material were subject of current research. Formation of TiB₂ and AlN was established in samples sintered at temperatures above 1750 °C. The highest values of microhardness were found in samples sintered at the temperature range of 1850 – 2000 °C. Fracture toughness of samples practically does not change during thermobaric sintering |
---|