Polymer composite materials with a high level of thermal stability based on phenolic resins and disperse silica fillers
Development of the engineering industry is difficult without using of heat-resistant polymer composite materials for manufacturing of machines and mechanisms parts operating at temperatures up to 300°C. For this purpose it was suggested the diphenylolsulfone formaldehyde resin as a polymer matrix, a...
Збережено в:
Дата: | 2018 |
---|---|
Автори: | , , , |
Формат: | Стаття |
Мова: | English |
Опубліковано: |
Інститут досліджень науково-технічного потенціалу та історії науки ім. Г.М. Доброва НАН України
2018
|
Назва видання: | Наука, технології, інновації |
Теми: | |
Онлайн доступ: | http://dspace.nbuv.gov.ua/handle/123456789/162628 |
Теги: |
Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
|
Назва журналу: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
Цитувати: | Polymer composite materials with a high level of thermal stability based on phenolic resins and disperse silica fillers / O.S. Kabat, Yu.M. Kobelchuk, D.O. Chervakov, O.V. Chervakov // Наука, технології, інновації. — 2018. — № 2 (6). — С. 48-53. — Бібліогр.: 25 назв. — англ. |
Репозитарії
Digital Library of Periodicals of National Academy of Sciences of UkraineРезюме: | Development of the engineering industry is difficult without using of heat-resistant polymer composite materials for manufacturing of machines and mechanisms parts operating at temperatures up to 300°C. For this purpose it was suggested the diphenylolsulfone formaldehyde resin as a polymer matrix, and different modifications of disperse silicas — white soot WS-120 and aerosol A-380 — were selected for fillers. The developed phenoplasts have high level of thermal stability (up to 370 °C), it’s at 25–30°C is higher, then for initial resins. Apparently, this is a result of increasing of the interaction level on the boundary “polymer-disperse filler”, under the processing condition (at temperatures 170–190°C) due to appearing of covalent and hydrogen bonds between hydroxyl groups at the surface of the silica and methylol groups of the polymer matrix. |
---|