Welding of defects in cast cases of turbines with perlite electrodes without heating and thermal processing

The regularities of structural formation of the weld metal and HAZ during multilayer welding, made by the transverse humping method, with short sections of defects on cast steel 15Kh1M1FL with perlite electrodes without heating and heat treatment are considered. It has been established that the stru...

Повний опис

Збережено в:
Бібліографічні деталі
Дата:2020
Автори: Efimenko, N.G., Artyomova, S.V.
Формат: Стаття
Мова:English
Опубліковано: Національний науковий центр «Харківський фізико-технічний інститут» НАН України 2020
Назва видання:Вопросы атомной науки и техники
Теми:
Онлайн доступ:http://dspace.nbuv.gov.ua/handle/123456789/194418
Теги: Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
Назва журналу:Digital Library of Periodicals of National Academy of Sciences of Ukraine
Цитувати:Welding of defects in cast cases of turbines with perlite electrodes without heating and thermal processing / N.G. Efimenko, S.V. Artyomova // Problems of atomic science and tecnology. — 2020. — № 4. — С. 84-88. — Бібліогр.: 15 назв. — англ.

Репозитарії

Digital Library of Periodicals of National Academy of Sciences of Ukraine
Опис
Резюме:The regularities of structural formation of the weld metal and HAZ during multilayer welding, made by the transverse humping method, with short sections of defects on cast steel 15Kh1M1FL with perlite electrodes without heating and heat treatment are considered. It has been established that the structure of all the studied zones of the welded joint is represented by upper granular bainite of varying degrees of dispersion. The difference in the hardness of the structures in the upper and middle parts of the welded joint is insignificant (3I4 and 296 HV, respectively). In the upper part, the formation of a hypereutectoid ferrite is found, which is located along the grain boundaries, which is also related with edge effect. The plastic properties of the weld metal are increased by more than 1.5 times, KCV – by more than 3 times in comparison with the base metal.