Improving the quality condition of the structure of welded joints made of rotor steel

The solution to the problem of increasing the reliability and service life of the welded joint of the rotor involved obtaining its original structure with improved quality characteristics. Obtaining was achieved by improving the technology of automatic welding. This improvement was based on the perf...

Повний опис

Збережено в:
Бібліографічні деталі
Видавець:Національний науковий центр «Харківський фізико-технічний інститут» НАН України
Дата:2022
Автори: Dmytryk, V.V., Skulsky, V.Yu., Kasyanenko, I.V., Vavilov, O.V., Kantor, O.G.
Формат: Стаття
Мова:English
Опубліковано: Національний науковий центр «Харківський фізико-технічний інститут» НАН України 2022
Назва видання:Вопросы атомной науки и техники
Теми:
Онлайн доступ:http://dspace.nbuv.gov.ua/handle/123456789/195931
Теги: Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
Цитувати:Improving the quality condition of the structure of welded joints made of rotor steel / V.V. Dmytryk, V.Yu. Skulsky, I.V. Kasyanenko, O.V. Vavilov, O.G. Kantor // Problems of Atomic Science and Technology. — 2022. — № 1. — С. 212-216. — Бібліогр.: 8 назв. — англ.

Репозиторії

Digital Library of Periodicals of National Academy of Sciences of Ukraine
Опис
Резюме:The solution to the problem of increasing the reliability and service life of the welded joint of the rotor involved obtaining its original structure with improved quality characteristics. Obtaining was achieved by improving the technology of automatic welding. This improvement was based on the performing the welding process on the optimized parameters of the mode, which provided the appropriate temperature regime of the one-piece connection that is made. Thus, the welding heat provided the formation of the original structure with higher quality characteristics in comparison with a similar structure obtained by the normal mode of welding. It was found that austenitic grains in the structure of the heat affected zone of the welded joint, which is heated above Аc₃, are smaller in size compared to similar grains in the structure of the standard technology. Accordingly, the new decay products of austenite in the area of heat affected zone, which is heated to the temperature range Ac₁–Ac₃, were sorbitol and troostite. In general, by obtaining a better structure allowed to increase the reliability and increase the service life of the rotor by 10…15%.