Dielectric permittivity of (Ag₃AsS₃)x(As₂S₃)₁₋x superionic glasses and composites

Complex dielectric permittivity of (Ag₃AsS₃)x(As₂S₃)₁₋x (x = 0.3−0.9) superionic glasses and composites at 300 K were studied. A decrease of the real part of dielectric permittivity with frequency by almost five orders of magnitude as well as one dispersion region in glasses and two dispersion re...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Datum:2014
Hauptverfasser: Studenyak, I.P., Neimet, Yu.Yu., Orliukas, A.F., Kežionis, A., Kazakevičius, E., Šalkus, T.
Format: Artikel
Sprache:English
Veröffentlicht: Інститут фізики напівпровідників імені В.Є. Лашкарьова НАН України 2014
Schriftenreihe:Semiconductor Physics Quantum Electronics & Optoelectronics
Online Zugang:https://nasplib.isofts.kiev.ua/handle/123456789/118368
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Назва журналу:Digital Library of Periodicals of National Academy of Sciences of Ukraine
Zitieren:Dielectric permittivity of (Ag₃AsS₃)x(As₂S₃)₁₋x superionic glasses and composites / I.P. Studenyak, Yu.Yu. Neimet, A.F. Orliukas, A. Kezionis, E. Kazakevicius, T. Salkus // Semiconductor Physics Quantum Electronics & Optoelectronics. — 2014. — Т. 17, № 2. — С. 174-178. — Бібліогр.: 20 назв. — англ.

Institution

Digital Library of Periodicals of National Academy of Sciences of Ukraine
Beschreibung
Zusammenfassung:Complex dielectric permittivity of (Ag₃AsS₃)x(As₂S₃)₁₋x (x = 0.3−0.9) superionic glasses and composites at 300 K were studied. A decrease of the real part of dielectric permittivity with frequency by almost five orders of magnitude as well as one dispersion region in glasses and two dispersion regions in composites, which is reflected in the dielectric loss spectra, were observed. Frequency dependences of dielectric permittivity within the range from 10 Hz to 3x109 Hz were analyzed in the framework of the Cole-Cole model. Compositional behaviour of Cole-Cole parameters in (Ag₃AsS₃)x(As₂S₃)₁₋x (x = 0.3−0.9) superionic glasses and composites was studied. The most substantial changes were observed with the transition from (Ag₃AsS₃)₀.₄(As₂S₃)₀.₆ glass to (Ag₃AsS₃)₀.₅(As₂S₃)₀.₅ composite and from (Ag₃AsS₃)₀.₆(As₂S₃)₀.₄ composite to (Ag₃AsS₃)₀.₈(As₂S₃)₀.₂ composite.