Ellipsometry examination of copper alloys with transitive metals

Electron structure of copper alloys with 3d transition metals (Fe, Co and Cr) have been studied basing on elliposometrical measurement of D and Y in wide spectral range hn = 1.0–4.95 eV. Spectral dependences of Cu-Cr alloys optical conductivity in wide range of chrome concentration (C = 2.5–30 at. %...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Datum:2004
Hauptverfasser: Filipov, Y.V., Staschuk, V.S., Poperenko, L.V., Vovchenko, V.V.
Format: Artikel
Sprache:English
Veröffentlicht: Інститут фізики напівпровідників імені В.Є. Лашкарьова НАН України 2004
Schriftenreihe:Semiconductor Physics Quantum Electronics & Optoelectronics
Online Zugang:https://nasplib.isofts.kiev.ua/handle/123456789/119126
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Назва журналу:Digital Library of Periodicals of National Academy of Sciences of Ukraine
Zitieren:Ellipsometry examination of copper alloys with transitive metals / Y.V. Filipov, V.S. Staschuk, L.V. Poperenko, V.V. Vovchenko // Semiconductor Physics Quantum Electronics & Optoelectronics. — 2004. — Т. 7, № 3. — С. 287-290. — Бібліогр.: 10 назв. — англ.

Institution

Digital Library of Periodicals of National Academy of Sciences of Ukraine
Beschreibung
Zusammenfassung:Electron structure of copper alloys with 3d transition metals (Fe, Co and Cr) have been studied basing on elliposometrical measurement of D and Y in wide spectral range hn = 1.0–4.95 eV. Spectral dependences of Cu-Cr alloys optical conductivity in wide range of chrome concentration (C = 2.5–30 at. %) have been minutely analyzed in this work. Ascertainment that in spectrums of studied alloys (and for copper alloys with other transitive metals) were observed basic band of pure Cu, in addition supplementary band in range 1-2 eV were observed too. Is shown that at small Cr concentrations (C < 5 at. %) alloy is forming a single band similar to copper, with insignificant dependence of Fermi level EF from impurity concentrations. Besides there was founded that in electron structure appear impurity bands situated between Fermi level and d-band of copper. They split on 0.4 eV as a result of spin-orbit interaction. At high impurity concentrations (CCr > 5 at. %) the alloys are heterogeneous mixtures of pure transitive metals and copper based solid solution.