Optical and scintillation properties of CsI:In crystals
The work is dedicated to study of optical and scintillation properties of CsI:In crystals. Using the Bridgeman method a concentration row of CsI:In single crystals was grown with the dopant content from 10⁻⁴ to 10⁻¹ mol. %. The segregation coefficient of In in CsI was estimated to be ~0.15. In...
Збережено в:
| Опубліковано в: : | Functional Materials |
|---|---|
| Дата: | 2013 |
| Автори: | , , , , , , |
| Формат: | Стаття |
| Мова: | English |
| Опубліковано: |
НТК «Інститут монокристалів» НАН України
2013
|
| Теми: | |
| Онлайн доступ: | https://nasplib.isofts.kiev.ua/handle/123456789/120077 |
| Теги: |
Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
|
| Назва журналу: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| Цитувати: | Optical and scintillation properties of CsI:In crystals / S. Gridin, N. Shiran, M. Moszynski, A. Belsky, A. Syntfeld-Kazuch, V. Tarasov, A. Gektin // Functional Materials. — 2013. — Т. 20, № 3. — С. 284-289. — Бібліогр.: 14 назв. — англ. |
Репозитарії
Digital Library of Periodicals of National Academy of Sciences of Ukraine| id |
nasplib_isofts_kiev_ua-123456789-120077 |
|---|---|
| record_format |
dspace |
| spelling |
Gridin, S. Shiran, N. Moszynski, M. Belsky, A. Syntfeld-Kazuch, A. Tarasov, V. Gektin, A. 2017-06-11T05:55:16Z 2017-06-11T05:55:16Z 2013 Optical and scintillation properties of CsI:In crystals / S. Gridin, N. Shiran, M. Moszynski, A. Belsky, A. Syntfeld-Kazuch, V. Tarasov, A. Gektin // Functional Materials. — 2013. — Т. 20, № 3. — С. 284-289. — Бібліогр.: 14 назв. — англ. 1027-5495 DOI: dx.doi.org/10.15407/fm20.03.284 https://nasplib.isofts.kiev.ua/handle/123456789/120077 The work is dedicated to study of optical and scintillation properties of CsI:In crystals. Using the Bridgeman method a concentration row of CsI:In single crystals was grown with the dopant content from 10⁻⁴ to 10⁻¹ mol. %. The segregation coefficient of In in CsI was estimated to be ~0.15. In CsI:In luminescence spectra one symmetric band is observed, peaking around 545 nm, with FWHM of 0.46 eV. Under intracenter excitation 1.9 μ s exponential decay was observed. The light yield under gamma excitation of ¹³⁷Cs isotope (662 keV), measured with a shaping time of 10 μ s, was 27 000 photons/MeV. The radio-luminescence yield of CsI:In , measured by the current mode method, approached to that of CsI:Tl . Probably, this difference is connected with the presence of a stronger afterglow in CsI:In crystals. en НТК «Інститут монокристалів» НАН України Functional Materials Characterization and properties Optical and scintillation properties of CsI:In crystals Article published earlier |
| institution |
Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| collection |
DSpace DC |
| title |
Optical and scintillation properties of CsI:In crystals |
| spellingShingle |
Optical and scintillation properties of CsI:In crystals Gridin, S. Shiran, N. Moszynski, M. Belsky, A. Syntfeld-Kazuch, A. Tarasov, V. Gektin, A. Characterization and properties |
| title_short |
Optical and scintillation properties of CsI:In crystals |
| title_full |
Optical and scintillation properties of CsI:In crystals |
| title_fullStr |
Optical and scintillation properties of CsI:In crystals |
| title_full_unstemmed |
Optical and scintillation properties of CsI:In crystals |
| title_sort |
optical and scintillation properties of csi:in crystals |
| author |
Gridin, S. Shiran, N. Moszynski, M. Belsky, A. Syntfeld-Kazuch, A. Tarasov, V. Gektin, A. |
| author_facet |
Gridin, S. Shiran, N. Moszynski, M. Belsky, A. Syntfeld-Kazuch, A. Tarasov, V. Gektin, A. |
| topic |
Characterization and properties |
| topic_facet |
Characterization and properties |
| publishDate |
2013 |
| language |
English |
| container_title |
Functional Materials |
| publisher |
НТК «Інститут монокристалів» НАН України |
| format |
Article |
| description |
The work is dedicated to study of optical and scintillation properties of CsI:In crystals. Using the Bridgeman method a concentration row of CsI:In single crystals was grown with the dopant content from 10⁻⁴ to 10⁻¹ mol. %. The segregation coefficient of In in CsI was estimated to be ~0.15. In CsI:In luminescence spectra one symmetric band is observed, peaking around 545 nm, with FWHM of 0.46 eV. Under intracenter excitation 1.9 μ s exponential decay was observed. The light yield under gamma excitation of ¹³⁷Cs isotope (662 keV), measured with a shaping time of 10 μ s, was 27 000 photons/MeV. The radio-luminescence yield of CsI:In , measured by the current mode method, approached to that of CsI:Tl . Probably, this difference is connected with the presence of a stronger afterglow in CsI:In crystals.
|
| issn |
1027-5495 |
| url |
https://nasplib.isofts.kiev.ua/handle/123456789/120077 |
| fulltext |
|
| citation_txt |
Optical and scintillation properties of CsI:In crystals / S. Gridin, N. Shiran, M. Moszynski, A. Belsky, A. Syntfeld-Kazuch, V. Tarasov, A. Gektin // Functional Materials. — 2013. — Т. 20, № 3. — С. 284-289. — Бібліогр.: 14 назв. — англ. |
| work_keys_str_mv |
AT gridins opticalandscintillationpropertiesofcsiincrystals AT shirann opticalandscintillationpropertiesofcsiincrystals AT moszynskim opticalandscintillationpropertiesofcsiincrystals AT belskya opticalandscintillationpropertiesofcsiincrystals AT syntfeldkazucha opticalandscintillationpropertiesofcsiincrystals AT tarasovv opticalandscintillationpropertiesofcsiincrystals AT gektina opticalandscintillationpropertiesofcsiincrystals |
| first_indexed |
2025-11-24T15:15:03Z |
| last_indexed |
2025-11-24T15:15:03Z |
| _version_ |
1850847929267388416 |