Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple

The course of removal of oxide ion admixtures (deoxidization) from molten cesium iodide using galvanic couple zirconium-platinum at 973 K was studied by a potentiometric method using a membrane oxygen electrode Pt(O₂)⁄YSZ (YSZ - yttria stabilized zirconia) as an indicator one for the detection of cu...

Повний опис

Збережено в:
Бібліографічні деталі
Опубліковано в: :Functional Materials
Дата:2016
Автори: Cherginets, V.L., Rebrova, T.P., Datsko, Y.N., Rebrov, A.L., Mateychenko, P.V.
Формат: Стаття
Мова:Англійська
Опубліковано: НТК «Інститут монокристалів» НАН України 2016
Теми:
Онлайн доступ:https://nasplib.isofts.kiev.ua/handle/123456789/121501
Теги: Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
Назва журналу:Digital Library of Periodicals of National Academy of Sciences of Ukraine
Цитувати:Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple / V.L. Cherginets, T.P. Rebrova, Y.N. Datsko,A.L. Rebrov, P.V. Mateychenko // Functional Materials. — 2016. — Т. 23, № 4. — С. 644-649. — Бібліогр.: 9 назв. — англ.

Репозитарії

Digital Library of Periodicals of National Academy of Sciences of Ukraine
_version_ 1862622432763838464
author Cherginets, V.L.
Rebrova, T.P.
Datsko, Y.N.
Rebrov, A.L.
Mateychenko, P.V.
author_facet Cherginets, V.L.
Rebrova, T.P.
Datsko, Y.N.
Rebrov, A.L.
Mateychenko, P.V.
citation_txt Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple / V.L. Cherginets, T.P. Rebrova, Y.N. Datsko,A.L. Rebrov, P.V. Mateychenko // Functional Materials. — 2016. — Т. 23, № 4. — С. 644-649. — Бібліогр.: 9 назв. — англ.
collection DSpace DC
container_title Functional Materials
description The course of removal of oxide ion admixtures (deoxidization) from molten cesium iodide using galvanic couple zirconium-platinum at 973 K was studied by a potentiometric method using a membrane oxygen electrode Pt(O₂)⁄YSZ (YSZ - yttria stabilized zirconia) as an indicator one for the detection of current and equilibrium concentrations of O₂-. The running of the deoxidization in both cases is subjected to kinetics of 2nd order process with respect to O<m^>2- and the rate constant is as (3.07±0.31)·106 kg·mol⁻¹·min⁻¹·cm⁻² for the galvanic couple. Surface capacity of the galvanic couple with respect to oxide ions was estimated as 7.6·10-4 mol·cm⁻². The destruction and fixation of oxygen-containing admixtures in the case of the galvanic couple occur more intensively that in the case of pure zirconium and Zr-Pt combination is more promising agent for deep purification of growth halide melts.
first_indexed 2025-12-07T13:27:51Z
format Article
fulltext
id nasplib_isofts_kiev_ua-123456789-121501
institution Digital Library of Periodicals of National Academy of Sciences of Ukraine
issn 1027-5495
language English
last_indexed 2025-12-07T13:27:51Z
publishDate 2016
publisher НТК «Інститут монокристалів» НАН України
record_format dspace
spelling Cherginets, V.L.
Rebrova, T.P.
Datsko, Y.N.
Rebrov, A.L.
Mateychenko, P.V.
2017-06-14T14:23:17Z
2017-06-14T14:23:17Z
2016
Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple / V.L. Cherginets, T.P. Rebrova, Y.N. Datsko,A.L. Rebrov, P.V. Mateychenko // Functional Materials. — 2016. — Т. 23, № 4. — С. 644-649. — Бібліогр.: 9 назв. — англ.
1027-5495
DOI: doi.org/10.15407/fm23.644
https://nasplib.isofts.kiev.ua/handle/123456789/121501
The course of removal of oxide ion admixtures (deoxidization) from molten cesium iodide using galvanic couple zirconium-platinum at 973 K was studied by a potentiometric method using a membrane oxygen electrode Pt(O₂)⁄YSZ (YSZ - yttria stabilized zirconia) as an indicator one for the detection of current and equilibrium concentrations of O₂-. The running of the deoxidization in both cases is subjected to kinetics of 2nd order process with respect to O<m^>2- and the rate constant is as (3.07±0.31)·106 kg·mol⁻¹·min⁻¹·cm⁻² for the galvanic couple. Surface capacity of the galvanic couple with respect to oxide ions was estimated as 7.6·10-4 mol·cm⁻². The destruction and fixation of oxygen-containing admixtures in the case of the galvanic couple occur more intensively that in the case of pure zirconium and Zr-Pt combination is more promising agent for deep purification of growth halide melts.
en
НТК «Інститут монокристалів» НАН України
Functional Materials
Technology
Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple
Article
published earlier
spellingShingle Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple
Cherginets, V.L.
Rebrova, T.P.
Datsko, Y.N.
Rebrov, A.L.
Mateychenko, P.V.
Technology
title Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple
title_full Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple
title_fullStr Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple
title_full_unstemmed Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple
title_short Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple
title_sort study of deoxidization process of csi melt by the action of "zr-pt" galvanic couple
topic Technology
topic_facet Technology
url https://nasplib.isofts.kiev.ua/handle/123456789/121501
work_keys_str_mv AT cherginetsvl studyofdeoxidizationprocessofcsimeltbytheactionofzrptgalvaniccouple
AT rebrovatp studyofdeoxidizationprocessofcsimeltbytheactionofzrptgalvaniccouple
AT datskoyn studyofdeoxidizationprocessofcsimeltbytheactionofzrptgalvaniccouple
AT rebroval studyofdeoxidizationprocessofcsimeltbytheactionofzrptgalvaniccouple
AT mateychenkopv studyofdeoxidizationprocessofcsimeltbytheactionofzrptgalvaniccouple