Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing
The processes at high temperature annealing of non-stoichiometric МgО·nАІ₂O₃ spinel crystals (n = 2.2) in O₂ atmosphere at 1300-1500°C have been investigated. A gradual non-stoichiometry increase up to n = 2.8 has been found with increasing annealing time due to MgO evaporation followed by formation...
Saved in:
| Published in: | Functional Materials |
|---|---|
| Date: | 2009 |
| Main Authors: | , , , |
| Format: | Article |
| Language: | English |
| Published: |
НТК «Інститут монокристалів» НАН України
2009
|
| Subjects: | |
| Online Access: | https://nasplib.isofts.kiev.ua/handle/123456789/138903 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Journal Title: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| Cite this: | Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing // G.I. Belykh, V.T. Gritsyna, L.A. Lytvynov, V.B. Kolner // Functional Materials. — 2009. — Т. 16, № 3. — С. 241-246. — Бібліогр.: 22 назв. — англ. |
Institution
Digital Library of Periodicals of National Academy of Sciences of Ukraine| _version_ | 1862716487876214784 |
|---|---|
| author | Belykh, G.I. Gritsyna, V.T. Lytvynov, L.A. Kolner, V.B. |
| author_facet | Belykh, G.I. Gritsyna, V.T. Lytvynov, L.A. Kolner, V.B. |
| citation_txt | Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing // G.I. Belykh, V.T. Gritsyna, L.A. Lytvynov, V.B. Kolner // Functional Materials. — 2009. — Т. 16, № 3. — С. 241-246. — Бібліогр.: 22 назв. — англ. |
| collection | DSpace DC |
| container_title | Functional Materials |
| description | The processes at high temperature annealing of non-stoichiometric МgО·nАІ₂O₃ spinel crystals (n = 2.2) in O₂ atmosphere at 1300-1500°C have been investigated. A gradual non-stoichiometry increase up to n = 2.8 has been found with increasing annealing time due to MgO evaporation followed by formation of polycrystalline α-АІ₂O₃ phase. The structure and composition МgО·nАІ₂O₃ layer grown at the sapphire surface in MgO vapor of at 1500-1800°C have been studied. The formation of amorphous phase in transition zone from hexagonal sapphire structure with a piling sequence ABABAB into spinel cubic one with sequence of atomic layers ABCABC was established.
Досліджено процеси високотемпературного відпалу нестехіометричних кристалів шпінелі МgО·nАІ₂O₃ в атмосфері O₂ при 1300-1500°С. Виявлено поступове збільшення нестехіометрії кристалів до п = 2,8 зі збільшенням часу відпалу внаслідок випаровування MgO з наступним формуванням полікристаличної фази α-АІ₂O₃. Досліджено структуру та склад шарів МgО·nАІ₂O₃, вирощених на поверхні сапфіру в парах MgO при 1500- 1800°С. Встановлено формування аморфної фази у зоні переходу від гексагональної структури сапфіру з послідовністю укладки шарів АВАВАВ у кубічну структуру шпінелі з послідовністю укладки атомних шарів АВСАВС.
Исследованы процессы высокотемпературного отжига кристаллов нестехиометрической шпинели МgО·nАІ₂O₃ (п = 2,2) в атмосфере O₂ при 1300-1500°С. Установлено постепенное увеличение нестехиометрии кристаллов до п = 2,8 с увеличением времени отжига вследствие испарения MgO и последующего образования поликристаллической фазы α-АІ₂O₃. Исследованы структура и состав слоев МgО·nАІ₂O₃, выращенных на поверхности сапфира в парах MgO при 1500-1800°С. Установлено формирование аморфной фазы в зоне перехода из гексагональной структуры сапфира с последовательностью укладки слоев АВАВАВ в кубическую структуру шпинели с последовательностью укладки атомных слоев АВСАВС.
|
| first_indexed | 2025-12-07T18:05:35Z |
| format | Article |
| fulltext | |
| id | nasplib_isofts_kiev_ua-123456789-138903 |
| institution | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| issn | 1027-5495 |
| language | English |
| last_indexed | 2025-12-07T18:05:35Z |
| publishDate | 2009 |
| publisher | НТК «Інститут монокристалів» НАН України |
| record_format | dspace |
| spelling | Belykh, G.I. Gritsyna, V.T. Lytvynov, L.A. Kolner, V.B. 2018-06-19T16:54:27Z 2018-06-19T16:54:27Z 2009 Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing // G.I. Belykh, V.T. Gritsyna, L.A. Lytvynov, V.B. Kolner // Functional Materials. — 2009. — Т. 16, № 3. — С. 241-246. — Бібліогр.: 22 назв. — англ. 1027-5495 https://nasplib.isofts.kiev.ua/handle/123456789/138903 The processes at high temperature annealing of non-stoichiometric МgО·nАІ₂O₃ spinel crystals (n = 2.2) in O₂ atmosphere at 1300-1500°C have been investigated. A gradual non-stoichiometry increase up to n = 2.8 has been found with increasing annealing time due to MgO evaporation followed by formation of polycrystalline α-АІ₂O₃ phase. The structure and composition МgО·nАІ₂O₃ layer grown at the sapphire surface in MgO vapor of at 1500-1800°C have been studied. The formation of amorphous phase in transition zone from hexagonal sapphire structure with a piling sequence ABABAB into spinel cubic one with sequence of atomic layers ABCABC was established. Досліджено процеси високотемпературного відпалу нестехіометричних кристалів шпінелі МgО·nАІ₂O₃ в атмосфері O₂ при 1300-1500°С. Виявлено поступове збільшення нестехіометрії кристалів до п = 2,8 зі збільшенням часу відпалу внаслідок випаровування MgO з наступним формуванням полікристаличної фази α-АІ₂O₃. Досліджено структуру та склад шарів МgО·nАІ₂O₃, вирощених на поверхні сапфіру в парах MgO при 1500- 1800°С. Встановлено формування аморфної фази у зоні переходу від гексагональної структури сапфіру з послідовністю укладки шарів АВАВАВ у кубічну структуру шпінелі з послідовністю укладки атомних шарів АВСАВС. Исследованы процессы высокотемпературного отжига кристаллов нестехиометрической шпинели МgО·nАІ₂O₃ (п = 2,2) в атмосфере O₂ при 1300-1500°С. Установлено постепенное увеличение нестехиометрии кристаллов до п = 2,8 с увеличением времени отжига вследствие испарения MgO и последующего образования поликристаллической фазы α-АІ₂O₃. Исследованы структура и состав слоев МgО·nАІ₂O₃, выращенных на поверхности сапфира в парах MgO при 1500-1800°С. Установлено формирование аморфной фазы в зоне перехода из гексагональной структуры сапфира с последовательностью укладки слоев АВАВАВ в кубическую структуру шпинели с последовательностью укладки атомных слоев АВСАВС. en НТК «Інститут монокристалів» НАН України Functional Materials Characterization and properties Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing Перетворення структури кристалів шпінелі МgО·nАІ₂O₃ при високотемпературному відпалі Article published earlier |
| spellingShingle | Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing Belykh, G.I. Gritsyna, V.T. Lytvynov, L.A. Kolner, V.B. Characterization and properties |
| title | Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing |
| title_alt | Перетворення структури кристалів шпінелі МgО·nАІ₂O₃ при високотемпературному відпалі |
| title_full | Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing |
| title_fullStr | Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing |
| title_full_unstemmed | Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing |
| title_short | Transformation of spinel crystals structure МgО·nАІ₂O₃ under high-temperature annealing |
| title_sort | transformation of spinel crystals structure мgо·nаі₂o₃ under high-temperature annealing |
| topic | Characterization and properties |
| topic_facet | Characterization and properties |
| url | https://nasplib.isofts.kiev.ua/handle/123456789/138903 |
| work_keys_str_mv | AT belykhgi transformationofspinelcrystalsstructuremgonaí2o3underhightemperatureannealing AT gritsynavt transformationofspinelcrystalsstructuremgonaí2o3underhightemperatureannealing AT lytvynovla transformationofspinelcrystalsstructuremgonaí2o3underhightemperatureannealing AT kolnervb transformationofspinelcrystalsstructuremgonaí2o3underhightemperatureannealing AT belykhgi peretvorennâstrukturikristalívšpínelímgonaí2o3privisokotemperaturnomuvídpalí AT gritsynavt peretvorennâstrukturikristalívšpínelímgonaí2o3privisokotemperaturnomuvídpalí AT lytvynovla peretvorennâstrukturikristalívšpínelímgonaí2o3privisokotemperaturnomuvídpalí AT kolnervb peretvorennâstrukturikristalívšpínelímgonaí2o3privisokotemperaturnomuvídpalí |