Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings
The effect of structure on nano-hardness and elastic modulus of Ti-W-B nanocrystalline coatings prepared by triode sputtering has been studied. The material structure state has been found to change from cluster-crystalline (at low sputtering potentials U = 0.6 to 1.0 kV) to preferentially oriented-c...
Збережено в:
| Опубліковано в: : | Functional Materials |
|---|---|
| Дата: | 2006 |
| Автори: | , , , , |
| Формат: | Стаття |
| Мова: | English |
| Опубліковано: |
НТК «Інститут монокристалів» НАН України
2006
|
| Онлайн доступ: | https://nasplib.isofts.kiev.ua/handle/123456789/139912 |
| Теги: |
Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
|
| Назва журналу: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| Цитувати: | Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings / O.V. Sobol', S.N. Dub, O.N. Grigor`ev, A.A. Podtelezhnikov, A.N. Stetsenko // Functional Materials. — 2006. — Т. 13, № 1. — С. 105-112. — Бібліогр.: 25 назв. — англ. |
Репозитарії
Digital Library of Periodicals of National Academy of Sciences of Ukraine| id |
nasplib_isofts_kiev_ua-123456789-139912 |
|---|---|
| record_format |
dspace |
| spelling |
Sobol', O.V. Dub, S.N. Grigor`ev, O.N. Podtelezhnikov, A.A. Stetsenko, A.N. 2018-06-21T13:39:11Z 2018-06-21T13:39:11Z 2006 Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings / O.V. Sobol', S.N. Dub, O.N. Grigor`ev, A.A. Podtelezhnikov, A.N. Stetsenko // Functional Materials. — 2006. — Т. 13, № 1. — С. 105-112. — Бібліогр.: 25 назв. — англ. 1027-5495 https://nasplib.isofts.kiev.ua/handle/123456789/139912 The effect of structure on nano-hardness and elastic modulus of Ti-W-B nanocrystalline coatings prepared by triode sputtering has been studied. The material structure state has been found to change from cluster-crystalline (at low sputtering potentials U = 0.6 to 1.0 kV) to preferentially oriented-crystalline (at U > 2.2 kV). The texture perfection improvement with increasing U results in increased hardness and elastic modulus of the condensates. The maximum values were attained at U = 3.2 kV and amounted Н = 19.9 GPa and Е = 205 GPa for the cubic phase and Н = 37.9 GPa, Е = 389 GPa for the hexagonal phase, respectively. Исследовано влияние структуры нанокристаллических Ti-W-B покрытий, полученных триодным распылением, на их нанотвердость и модуль упругости. Выявлено изменение структурного состояния материала от кластерно-кристаллического при низких значениях распыляющего напряжения U = 0,6...1,0 кB до преимущественно ориентированного-кристаллического при U > 2,2 кВ. Рост совершенства текстуры с увеличением U приводит к повышению твердости и модуля упругости конденсатов. Максимальные значения были достигнуты при U = 3,2 кB и составляют для фазы с кубической решеткой: твердость Н = 19,9 ГПа, модуль упругости Е = 205 ГПа, а для фазы с гексагональной решеткой: Н = 37,9 ГПа, Е = 389 ГПа. Дослiджено вплив структури нанокристалiчних Ti-W-B iонно-плазмових (трiодна схема) покриттiв на їх нанотвердiсть та модуль пружностi. Виявлено змiни структурного стану матерiалу вiд кластерно-кристалiчного при низьких значеннях U = 0,6...1,0 кВ до переважно орiєнтованого кристалiчного при U > 2,2 кВ. 3ростання досконалостi текстури зi збiльшенням U призводить до зростання твердостi та модулю пружностi конденсатiв. Максимальнi значення досягнуто при U = 3,2 кВ i складають для фази з кубiчною граткою: твердiсть Н = 19,9 ГПа, модуль пружностi Е = 205 ГПа, а для фази з гексагональною граткою: Н = 37,9 ГПа, Е = 389 ГПа. en НТК «Інститут монокристалів» НАН України Functional Materials Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings Вплив структурного стану на механічні властивості нанокристалічних покриттів системи Ti-W-B Article published earlier |
| institution |
Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| collection |
DSpace DC |
| title |
Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings |
| spellingShingle |
Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings Sobol', O.V. Dub, S.N. Grigor`ev, O.N. Podtelezhnikov, A.A. Stetsenko, A.N. |
| title_short |
Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings |
| title_full |
Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings |
| title_fullStr |
Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings |
| title_full_unstemmed |
Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings |
| title_sort |
structure influence on mechanical properties of ti-w-b system nanocrystalline coatings |
| author |
Sobol', O.V. Dub, S.N. Grigor`ev, O.N. Podtelezhnikov, A.A. Stetsenko, A.N. |
| author_facet |
Sobol', O.V. Dub, S.N. Grigor`ev, O.N. Podtelezhnikov, A.A. Stetsenko, A.N. |
| publishDate |
2006 |
| language |
English |
| container_title |
Functional Materials |
| publisher |
НТК «Інститут монокристалів» НАН України |
| format |
Article |
| title_alt |
Вплив структурного стану на механічні властивості нанокристалічних покриттів системи Ti-W-B |
| description |
The effect of structure on nano-hardness and elastic modulus of Ti-W-B nanocrystalline coatings prepared by triode sputtering has been studied. The material structure state has been found to change from cluster-crystalline (at low sputtering potentials U = 0.6 to 1.0 kV) to preferentially oriented-crystalline (at U > 2.2 kV). The texture perfection improvement with increasing U results in increased hardness and elastic modulus of the condensates. The maximum values were attained at U = 3.2 kV and amounted Н = 19.9 GPa and Е = 205 GPa for the cubic phase and Н = 37.9 GPa, Е = 389 GPa for the hexagonal phase, respectively.
Исследовано влияние структуры нанокристаллических Ti-W-B покрытий, полученных триодным распылением, на их нанотвердость и модуль упругости. Выявлено изменение структурного состояния материала от кластерно-кристаллического при низких значениях распыляющего напряжения U = 0,6...1,0 кB до преимущественно ориентированного-кристаллического при U > 2,2 кВ. Рост совершенства текстуры с увеличением U приводит к повышению твердости и модуля упругости конденсатов. Максимальные значения были достигнуты при U = 3,2 кB и составляют для фазы с кубической решеткой: твердость Н = 19,9 ГПа, модуль упругости Е = 205 ГПа, а для фазы с гексагональной решеткой: Н = 37,9 ГПа, Е = 389 ГПа.
Дослiджено вплив структури нанокристалiчних Ti-W-B iонно-плазмових (трiодна схема) покриттiв на їх нанотвердiсть та модуль пружностi. Виявлено змiни структурного стану матерiалу вiд кластерно-кристалiчного при низьких значеннях U = 0,6...1,0 кВ до переважно орiєнтованого кристалiчного при U > 2,2 кВ. 3ростання досконалостi текстури зi збiльшенням U призводить до зростання твердостi та модулю пружностi конденсатiв. Максимальнi значення досягнуто при U = 3,2 кВ i складають для фази з кубiчною граткою: твердiсть Н = 19,9 ГПа, модуль пружностi Е = 205 ГПа, а для фази з гексагональною граткою: Н = 37,9 ГПа, Е = 389 ГПа.
|
| issn |
1027-5495 |
| url |
https://nasplib.isofts.kiev.ua/handle/123456789/139912 |
| citation_txt |
Structure influence on mechanical properties of Ti-W-B system nanocrystalline coatings / O.V. Sobol', S.N. Dub, O.N. Grigor`ev, A.A. Podtelezhnikov, A.N. Stetsenko // Functional Materials. — 2006. — Т. 13, № 1. — С. 105-112. — Бібліогр.: 25 назв. — англ. |
| work_keys_str_mv |
AT sobolov structureinfluenceonmechanicalpropertiesoftiwbsystemnanocrystallinecoatings AT dubsn structureinfluenceonmechanicalpropertiesoftiwbsystemnanocrystallinecoatings AT grigorevon structureinfluenceonmechanicalpropertiesoftiwbsystemnanocrystallinecoatings AT podtelezhnikovaa structureinfluenceonmechanicalpropertiesoftiwbsystemnanocrystallinecoatings AT stetsenkoan structureinfluenceonmechanicalpropertiesoftiwbsystemnanocrystallinecoatings AT sobolov vplivstrukturnogostanunamehaníčnívlastivostínanokristalíčnihpokrittívsistemitiwb AT dubsn vplivstrukturnogostanunamehaníčnívlastivostínanokristalíčnihpokrittívsistemitiwb AT grigorevon vplivstrukturnogostanunamehaníčnívlastivostínanokristalíčnihpokrittívsistemitiwb AT podtelezhnikovaa vplivstrukturnogostanunamehaníčnívlastivostínanokristalíčnihpokrittívsistemitiwb AT stetsenkoan vplivstrukturnogostanunamehaníčnívlastivostínanokristalíčnihpokrittívsistemitiwb |
| first_indexed |
2025-11-27T21:24:55Z |
| last_indexed |
2025-11-27T21:24:55Z |
| _version_ |
1850852851343949824 |