Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells

The optimization of the ITO frontal electrodes for flexible solar сells on CdTe base was carried out by annealing in air at 430℃. It has been shown, that for "superstrate" ITO/CdS/CdTe/Cu/Au solar cells, the preliminary annealing of ITO films provides the efficiency increase from 8.5 % up...

Full description

Saved in:
Bibliographic Details
Published in:Functional Materials
Date:2006
Main Author: Khrypunov, G.S.
Format: Article
Language:English
Published: НТК «Інститут монокристалів» НАН України 2006
Online Access:https://nasplib.isofts.kiev.ua/handle/123456789/139934
Tags: Add Tag
No Tags, Be the first to tag this record!
Journal Title:Digital Library of Periodicals of National Academy of Sciences of Ukraine
Cite this:Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells / G.S. Khrypunov // Functional Materials. — 2006. — Т. 13, № 1. — С. 113-118. — Бібліогр.: 14 назв. — англ.

Institution

Digital Library of Periodicals of National Academy of Sciences of Ukraine
id nasplib_isofts_kiev_ua-123456789-139934
record_format dspace
spelling Khrypunov, G.S.
2018-06-21T13:51:57Z
2018-06-21T13:51:57Z
2006
Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells / G.S. Khrypunov // Functional Materials. — 2006. — Т. 13, № 1. — С. 113-118. — Бібліогр.: 14 назв. — англ.
1027-5495
https://nasplib.isofts.kiev.ua/handle/123456789/139934
The optimization of the ITO frontal electrodes for flexible solar сells on CdTe base was carried out by annealing in air at 430℃. It has been shown, that for "superstrate" ITO/CdS/CdTe/Cu/Au solar cells, the preliminary annealing of ITO films provides the efficiency increase from 8.5 % up to 11.3 %, while for NaCl/ITO/CdS/CdTe/Cu/Au "substrate" solar cells, from 2.2 % up to 7.8 %.
Шляхом вiдпалу на повiтрi при температурi 430℃ виконано оптимiзацiю фронтального електроду ITO для гнучких плiвкових сонячних елементiв на основi телуриду кадмiю. Показано, що для сонячних елементiв ITO/CdS/CdTe/Cu/Au (типу "superstrate") попереднiй вiдпал шарiв ITO забезпечує зростання ефективностi вiд 8.5 % до 11.3 %, для сонячних елементiв NaCl/ITO/CdS/CdTe/Cu/Au (типу "substrate") вiд 2.2 % до 7.8 %.
Путем отжига на воздухе при температуре 430℃ проведена оптимизация фронтальных электродов ITO для гибких солнечных элементов на основе теллурида кадмия. Показано, что для солнечных элементов ITO/CdS/CdTe/Cu/Au (типа "superstrate") предварительный отжиг слоев ITO обеспечивает рост эффективности от 8,5 % до 11,3 %, а для солнечных элементов NaCl/ITO/CdS/CdTe/Cu/Au (типа "substrate") от 2,2 % до 7,8 %.
en
НТК «Інститут монокристалів» НАН України
Functional Materials
Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells
Оптимізація фронтальних електродів з ITO для гнучких плівкових сонячних елементів на основі CdTe
Article
published earlier
institution Digital Library of Periodicals of National Academy of Sciences of Ukraine
collection DSpace DC
title Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells
spellingShingle Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells
Khrypunov, G.S.
title_short Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells
title_full Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells
title_fullStr Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells
title_full_unstemmed Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells
title_sort optimization of the ito frontal electrodes for flexible cdte thin film solar cells
author Khrypunov, G.S.
author_facet Khrypunov, G.S.
publishDate 2006
language English
container_title Functional Materials
publisher НТК «Інститут монокристалів» НАН України
format Article
title_alt Оптимізація фронтальних електродів з ITO для гнучких плівкових сонячних елементів на основі CdTe
description The optimization of the ITO frontal electrodes for flexible solar сells on CdTe base was carried out by annealing in air at 430℃. It has been shown, that for "superstrate" ITO/CdS/CdTe/Cu/Au solar cells, the preliminary annealing of ITO films provides the efficiency increase from 8.5 % up to 11.3 %, while for NaCl/ITO/CdS/CdTe/Cu/Au "substrate" solar cells, from 2.2 % up to 7.8 %. Шляхом вiдпалу на повiтрi при температурi 430℃ виконано оптимiзацiю фронтального електроду ITO для гнучких плiвкових сонячних елементiв на основi телуриду кадмiю. Показано, що для сонячних елементiв ITO/CdS/CdTe/Cu/Au (типу "superstrate") попереднiй вiдпал шарiв ITO забезпечує зростання ефективностi вiд 8.5 % до 11.3 %, для сонячних елементiв NaCl/ITO/CdS/CdTe/Cu/Au (типу "substrate") вiд 2.2 % до 7.8 %. Путем отжига на воздухе при температуре 430℃ проведена оптимизация фронтальных электродов ITO для гибких солнечных элементов на основе теллурида кадмия. Показано, что для солнечных элементов ITO/CdS/CdTe/Cu/Au (типа "superstrate") предварительный отжиг слоев ITO обеспечивает рост эффективности от 8,5 % до 11,3 %, а для солнечных элементов NaCl/ITO/CdS/CdTe/Cu/Au (типа "substrate") от 2,2 % до 7,8 %.
issn 1027-5495
url https://nasplib.isofts.kiev.ua/handle/123456789/139934
citation_txt Optimization of the ITO frontal electrodes for flexible CdTe thin film solar cells / G.S. Khrypunov // Functional Materials. — 2006. — Т. 13, № 1. — С. 113-118. — Бібліогр.: 14 назв. — англ.
work_keys_str_mv AT khrypunovgs optimizationoftheitofrontalelectrodesforflexiblecdtethinfilmsolarcells
AT khrypunovgs optimízacíâfrontalʹnihelektrodívzitodlâgnučkihplívkovihsonâčnihelementívnaosnovícdte
first_indexed 2025-12-07T17:02:45Z
last_indexed 2025-12-07T17:02:45Z
_version_ 1850869773447987200