Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method

A sol-gel method has been developed to synthesize the binary system solid solutions of rare-earth elements manganites (1-x)La₀,₆Pb₀,₄MnO₃- xNd₀,₆(Sr₀,₇Pb₀,₃)₀,₄MnO₃ (x = 0, 0.5 and 1.0). X-ray investigations show that the formation of solid solution phase for all x was observed after annealing of xe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Functional Materials
Datum:2006
Hauptverfasser: Shitchkova, T.A., Emello, G.G., Bashkirov, L.A.
Format: Artikel
Sprache:English
Veröffentlicht: НТК «Інститут монокристалів» НАН України 2006
Online Zugang:https://nasplib.isofts.kiev.ua/handle/123456789/144384
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Назва журналу:Digital Library of Periodicals of National Academy of Sciences of Ukraine
Zitieren:Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method / T.A. Shitchkova, G.G. Emello, L.A. Bashkirov // Functional Materials. — 2006. — Т. 13, № 2. — С. 350-354. — Бібліогр.: 11 назв. — англ.

Institution

Digital Library of Periodicals of National Academy of Sciences of Ukraine
id nasplib_isofts_kiev_ua-123456789-144384
record_format dspace
spelling Shitchkova, T.A.
Emello, G.G.
Bashkirov, L.A.
2018-12-20T20:16:31Z
2018-12-20T20:16:31Z
2006
Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method / T.A. Shitchkova, G.G. Emello, L.A. Bashkirov // Functional Materials. — 2006. — Т. 13, № 2. — С. 350-354. — Бібліогр.: 11 назв. — англ.
1027-5495
https://nasplib.isofts.kiev.ua/handle/123456789/144384
A sol-gel method has been developed to synthesize the binary system solid solutions of rare-earth elements manganites (1-x)La₀,₆Pb₀,₄MnO₃- xNd₀,₆(Sr₀,₇Pb₀,₃)₀,₄MnO₃ (x = 0, 0.5 and 1.0). X-ray investigations show that the formation of solid solution phase for all x was observed after annealing of xerogel powders (tablets) in air at 700°C for 1 h. At x = 0.5 and 1.0, the solid solutions have an orthorhombically distorted perovskite structure, whereas at x = 0 (pure La₀,₆Pb₀,₄MnO₃), the crystal lattice is hexagonal. The specific saturation magnetization at 100 K (σ₁₀₀) and the Curie temperature (Tc) for manganite solid solutions synthesized using the sol-gel method (annealing at 900-1100°C for 1 h) at any x exceed the corresponding characteristics of similar solid solutions obtained by ceramic method (after 6 h heating at 1200 K).
Разработан золь-гель метод для синтеза твердых растворов двойной системы манганитов редкоземельных элементов 1-x)La₀,₆Pb₀,₄MnO₃- xNd₀,₆(Sr₀,₇Pb₀,₃)₀,₄MnO₃ (х = 0, 0,5 и 1,0). С помощью рентгенофазового анализа установлено, что независимо от состава образование фазы твердого раствора манганита со структурой перовскита наблюдается после обжига соответствующих по составу порошков ксерогелей (таблеток) на воздухе при 700°С в течение всего 1 часа. Установлено, что упомянутые твердые растворы при х = 0,5 и 1,0 имеют орторомбически искаженную структуру перовскита, а при х = 0 (La₀,₆Pb₀,₄MnO₃) кристаллическая решетка имеет гексагональную симметрию. Удельная намагниченность насыщения при 100 К (σ₁₀₀) и температура Кюри (Г,.) для синтезированных с использованием золь-гель технологии твердых растворов манганитов (обжиг при 900-1100°С в течение 1 ч) при любом составе были выше, чем эти же характеристики для твердых растворов аналогичных составов, синтезированных керамическим методом (обжиг при 1200 К в течение 6 ч).
Розроблено золь-гелевий метод для синтезу твердих розчинів подвійної системи манганітів рідкоземельних елементів 1-x)La₀,₆Pb₀,₄MnO₃- xNd₀,₆(Sr₀,₇Pb₀,₃)₀,₄MnO₃ (х = 0, 0,5 и 1,0). За допомогою рентгенофазового аналізу встановлено, що незалежно від складу утворення фази твердого розчину манганіту зі структурою перовскіту спостерігається після випалу відповідних за складом порошків ксерогелів (таблеток) на повітрі при 700°С протягом лише 1 години. Встановлено, що згадані тверді розчини при х = 0,5 та 1,0 мають орторомбічно спотворену структуру перовскіту, а при х = 0 (La₀,₆Pb₀,₄MnO₃) кристалічна гратка має гексагональну симетрію. Питома намагниченість насичення при 100 К (σ₁₀₀) та температура Кюрі (Тс) для синтезованих з застосуванням золь-гель технології твердих розчинів манганітів (випал при 900-1100°С протягом 1 год) при будь-якому складі були вище, ніж ті самі характеристики для аналогічних за складом твердих розчинів, синтезованих керамічним методом (випал при 1200 К протягом 6 год).
en
НТК «Інститут монокристалів» НАН України
Functional Materials
Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method
Синтез твердих розчинів Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' та Me'':Sr, Pb) з застосуванням золь-гелевого методу
Article
published earlier
institution Digital Library of Periodicals of National Academy of Sciences of Ukraine
collection DSpace DC
title Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method
spellingShingle Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method
Shitchkova, T.A.
Emello, G.G.
Bashkirov, L.A.
title_short Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method
title_full Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method
title_fullStr Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method
title_full_unstemmed Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method
title_sort synthesis of ln1-x-yme'xme''ymno₃ (ln:la, nd; me' and me'':sr, pb) solid solutions using sol-gel method
author Shitchkova, T.A.
Emello, G.G.
Bashkirov, L.A.
author_facet Shitchkova, T.A.
Emello, G.G.
Bashkirov, L.A.
publishDate 2006
language English
container_title Functional Materials
publisher НТК «Інститут монокристалів» НАН України
format Article
title_alt Синтез твердих розчинів Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' та Me'':Sr, Pb) з застосуванням золь-гелевого методу
description A sol-gel method has been developed to synthesize the binary system solid solutions of rare-earth elements manganites (1-x)La₀,₆Pb₀,₄MnO₃- xNd₀,₆(Sr₀,₇Pb₀,₃)₀,₄MnO₃ (x = 0, 0.5 and 1.0). X-ray investigations show that the formation of solid solution phase for all x was observed after annealing of xerogel powders (tablets) in air at 700°C for 1 h. At x = 0.5 and 1.0, the solid solutions have an orthorhombically distorted perovskite structure, whereas at x = 0 (pure La₀,₆Pb₀,₄MnO₃), the crystal lattice is hexagonal. The specific saturation magnetization at 100 K (σ₁₀₀) and the Curie temperature (Tc) for manganite solid solutions synthesized using the sol-gel method (annealing at 900-1100°C for 1 h) at any x exceed the corresponding characteristics of similar solid solutions obtained by ceramic method (after 6 h heating at 1200 K). Разработан золь-гель метод для синтеза твердых растворов двойной системы манганитов редкоземельных элементов 1-x)La₀,₆Pb₀,₄MnO₃- xNd₀,₆(Sr₀,₇Pb₀,₃)₀,₄MnO₃ (х = 0, 0,5 и 1,0). С помощью рентгенофазового анализа установлено, что независимо от состава образование фазы твердого раствора манганита со структурой перовскита наблюдается после обжига соответствующих по составу порошков ксерогелей (таблеток) на воздухе при 700°С в течение всего 1 часа. Установлено, что упомянутые твердые растворы при х = 0,5 и 1,0 имеют орторомбически искаженную структуру перовскита, а при х = 0 (La₀,₆Pb₀,₄MnO₃) кристаллическая решетка имеет гексагональную симметрию. Удельная намагниченность насыщения при 100 К (σ₁₀₀) и температура Кюри (Г,.) для синтезированных с использованием золь-гель технологии твердых растворов манганитов (обжиг при 900-1100°С в течение 1 ч) при любом составе были выше, чем эти же характеристики для твердых растворов аналогичных составов, синтезированных керамическим методом (обжиг при 1200 К в течение 6 ч). Розроблено золь-гелевий метод для синтезу твердих розчинів подвійної системи манганітів рідкоземельних елементів 1-x)La₀,₆Pb₀,₄MnO₃- xNd₀,₆(Sr₀,₇Pb₀,₃)₀,₄MnO₃ (х = 0, 0,5 и 1,0). За допомогою рентгенофазового аналізу встановлено, що незалежно від складу утворення фази твердого розчину манганіту зі структурою перовскіту спостерігається після випалу відповідних за складом порошків ксерогелів (таблеток) на повітрі при 700°С протягом лише 1 години. Встановлено, що згадані тверді розчини при х = 0,5 та 1,0 мають орторомбічно спотворену структуру перовскіту, а при х = 0 (La₀,₆Pb₀,₄MnO₃) кристалічна гратка має гексагональну симетрію. Питома намагниченість насичення при 100 К (σ₁₀₀) та температура Кюрі (Тс) для синтезованих з застосуванням золь-гель технології твердих розчинів манганітів (випал при 900-1100°С протягом 1 год) при будь-якому складі були вище, ніж ті самі характеристики для аналогічних за складом твердих розчинів, синтезованих керамічним методом (випал при 1200 К протягом 6 год).
issn 1027-5495
url https://nasplib.isofts.kiev.ua/handle/123456789/144384
citation_txt Synthesis of Ln1-x-yMe'xMe''yMnO₃ (Ln:La, Nd; Me' and Me'':Sr, Pb) solid solutions using sol-gel method / T.A. Shitchkova, G.G. Emello, L.A. Bashkirov // Functional Materials. — 2006. — Т. 13, № 2. — С. 350-354. — Бібліогр.: 11 назв. — англ.
work_keys_str_mv AT shitchkovata synthesisofln1xymexmeymno3lnlandmeandmesrpbsolidsolutionsusingsolgelmethod
AT emellogg synthesisofln1xymexmeymno3lnlandmeandmesrpbsolidsolutionsusingsolgelmethod
AT bashkirovla synthesisofln1xymexmeymno3lnlandmeandmesrpbsolidsolutionsusingsolgelmethod
AT shitchkovata sinteztverdihrozčinívln1xymexmeymno3lnlandmetamesrpbzzastosuvannâmzolʹgelevogometodu
AT emellogg sinteztverdihrozčinívln1xymexmeymno3lnlandmetamesrpbzzastosuvannâmzolʹgelevogometodu
AT bashkirovla sinteztverdihrozčinívln1xymexmeymno3lnlandmetamesrpbzzastosuvannâmzolʹgelevogometodu
first_indexed 2025-12-07T16:50:46Z
last_indexed 2025-12-07T16:50:46Z
_version_ 1850869019153793024