Structure and properties of solid BK6-OM alloy after electrosintering
In the paper we describe the results of the structure formation and physicomechanical properties of WC-Co hard alloy from he standard especially fine-grained BK6-OM mixture of KZTS (Russia) in electrosintering (ES) process with the use of a constant electric current (I = 3000 A) in a graphite mold i...
Saved in:
| Published in: | Functional Materials |
|---|---|
| Date: | 2018 |
| Main Authors: | , , , , |
| Format: | Article |
| Language: | English |
| Published: |
НТК «Інститут монокристалів» НАН України
2018
|
| Subjects: | |
| Online Access: | https://nasplib.isofts.kiev.ua/handle/123456789/157127 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Journal Title: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| Cite this: | Structure and properties of solid BK6-OM alloy after electrosintering / N.M. Prokopiv, E.S. Gevorkyan, R.V. Vovk, O.V. Harchenko, V.A. Chishkala // Functional Materials. — 2018. — Т. 25, № 2. — С. 267-273. — Бібліогр.: 27 назв. — англ. |
Institution
Digital Library of Periodicals of National Academy of Sciences of Ukraine| _version_ | 1862599507840073728 |
|---|---|
| author | Prokopiv, N.M. Gevorkyan, E.S. Vovk, R.V. Harchenko, O.V. Chishkala, V.A. |
| author_facet | Prokopiv, N.M. Gevorkyan, E.S. Vovk, R.V. Harchenko, O.V. Chishkala, V.A. |
| citation_txt | Structure and properties of solid BK6-OM alloy after electrosintering / N.M. Prokopiv, E.S. Gevorkyan, R.V. Vovk, O.V. Harchenko, V.A. Chishkala // Functional Materials. — 2018. — Т. 25, № 2. — С. 267-273. — Бібліогр.: 27 назв. — англ. |
| collection | DSpace DC |
| container_title | Functional Materials |
| description | In the paper we describe the results of the structure formation and physicomechanical properties of WC-Co hard alloy from he standard especially fine-grained BK6-OM mixture of KZTS (Russia) in electrosintering (ES) process with the use of a constant electric current (I = 3000 A) in a graphite mold in vacuum under pressure of 40 MPa and temperatures above (1320°C) and below (1220°C) of the solidus line of phase diagram. For comparison, samples from this mixture are sintered according to the standard technology in vacuum. The advantage of ES in conditions of the solid phase interaction (1200°C) is shown for obtaining the two-phase structure of hard alloy with high-density, without signs of recrystallization of carbide grains, from the standard mixture of BK6-OM, which increases by 30 % the thermal conductivity, hardness, and fracture toughness compared to the Sun. The mechanism of destruction of the samples after ES in conditions of impact loading is established.
|
| first_indexed | 2025-11-27T22:44:24Z |
| format | Article |
| fulltext | |
| id | nasplib_isofts_kiev_ua-123456789-157127 |
| institution | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| issn | 1027-5495 |
| language | English |
| last_indexed | 2025-11-27T22:44:24Z |
| publishDate | 2018 |
| publisher | НТК «Інститут монокристалів» НАН України |
| record_format | dspace |
| spelling | Prokopiv, N.M. Gevorkyan, E.S. Vovk, R.V. Harchenko, O.V. Chishkala, V.A. 2019-06-19T16:15:40Z 2019-06-19T16:15:40Z 2018 Structure and properties of solid BK6-OM alloy after electrosintering / N.M. Prokopiv, E.S. Gevorkyan, R.V. Vovk, O.V. Harchenko, V.A. Chishkala // Functional Materials. — 2018. — Т. 25, № 2. — С. 267-273. — Бібліогр.: 27 назв. — англ. 1027-5495 DOI:https://doi.org/10.15407/fm25.02.267 https://nasplib.isofts.kiev.ua/handle/123456789/157127 In the paper we describe the results of the structure formation and physicomechanical properties of WC-Co hard alloy from he standard especially fine-grained BK6-OM mixture of KZTS (Russia) in electrosintering (ES) process with the use of a constant electric current (I = 3000 A) in a graphite mold in vacuum under pressure of 40 MPa and temperatures above (1320°C) and below (1220°C) of the solidus line of phase diagram. For comparison, samples from this mixture are sintered according to the standard technology in vacuum. The advantage of ES in conditions of the solid phase interaction (1200°C) is shown for obtaining the two-phase structure of hard alloy with high-density, without signs of recrystallization of carbide grains, from the standard mixture of BK6-OM, which increases by 30 % the thermal conductivity, hardness, and fracture toughness compared to the Sun. The mechanism of destruction of the samples after ES in conditions of impact loading is established. en НТК «Інститут монокристалів» НАН України Functional Materials Characterization and properties Structure and properties of solid BK6-OM alloy after electrosintering Article published earlier |
| spellingShingle | Structure and properties of solid BK6-OM alloy after electrosintering Prokopiv, N.M. Gevorkyan, E.S. Vovk, R.V. Harchenko, O.V. Chishkala, V.A. Characterization and properties |
| title | Structure and properties of solid BK6-OM alloy after electrosintering |
| title_full | Structure and properties of solid BK6-OM alloy after electrosintering |
| title_fullStr | Structure and properties of solid BK6-OM alloy after electrosintering |
| title_full_unstemmed | Structure and properties of solid BK6-OM alloy after electrosintering |
| title_short | Structure and properties of solid BK6-OM alloy after electrosintering |
| title_sort | structure and properties of solid bk6-om alloy after electrosintering |
| topic | Characterization and properties |
| topic_facet | Characterization and properties |
| url | https://nasplib.isofts.kiev.ua/handle/123456789/157127 |
| work_keys_str_mv | AT prokopivnm structureandpropertiesofsolidbk6omalloyafterelectrosintering AT gevorkyanes structureandpropertiesofsolidbk6omalloyafterelectrosintering AT vovkrv structureandpropertiesofsolidbk6omalloyafterelectrosintering AT harchenkoov structureandpropertiesofsolidbk6omalloyafterelectrosintering AT chishkalava structureandpropertiesofsolidbk6omalloyafterelectrosintering |