cBN based materials with TiN-Al binder phase: sintering, structure, properties
Cubic boron nitride material was produced via high pressure and high temperature sintering with titanium nitride and aluminum as binder phase. Microstructure, phase composition and physical-mechanical properties of the material were subject of current research. Formation of TiB₂ and AlN was establis...
Saved in:
| Published in: | Породоразрушающий и металлообрабатывающий инструмент – техника и технология его изготовления и применения |
|---|---|
| Date: | 2019 |
| Main Authors: | , , , |
| Format: | Article |
| Language: | English |
| Published: |
Інститут надтвердих матеріалів ім. В.М. Бакуля НАН України
2019
|
| Subjects: | |
| Online Access: | https://nasplib.isofts.kiev.ua/handle/123456789/159970 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Journal Title: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| Cite this: | cBN based materials with TiN-Al binder phase: sintering, structure, properties / K.V. Slipchenko, V.Z. Turkevich, V.M. Bushlya, J.-E. Ståhl // Породоразрушающий и металлообрабатывающий инструмент – техника и технология его изготовления и применения: Сб. науч. тр. — К.: ІНМ ім. В.М. Бакуля НАН України, 2019. — Вип. 22. — С. 254-260. — Бібліогр.: 14 назв. — англ. |
Institution
Digital Library of Periodicals of National Academy of Sciences of Ukraine| id |
nasplib_isofts_kiev_ua-123456789-159970 |
|---|---|
| record_format |
dspace |
| spelling |
Slipchenko, K.V. Turkevich, V.Z. Bushlya, V.M. Ståhl, J.-E. 2019-10-19T16:47:53Z 2019-10-19T16:47:53Z 2019 cBN based materials with TiN-Al binder phase: sintering, structure, properties / K.V. Slipchenko, V.Z. Turkevich, V.M. Bushlya, J.-E. Ståhl // Породоразрушающий и металлообрабатывающий инструмент – техника и технология его изготовления и применения: Сб. науч. тр. — К.: ІНМ ім. В.М. Бакуля НАН України, 2019. — Вип. 22. — С. 254-260. — Бібліогр.: 14 назв. — англ. 2223-3938 DOI: 10.33839/2223-3938-2019-22-1-254-260 https://nasplib.isofts.kiev.ua/handle/123456789/159970 666.792.3 Cubic boron nitride material was produced via high pressure and high temperature sintering with titanium nitride and aluminum as binder phase. Microstructure, phase composition and physical-mechanical properties of the material were subject of current research. Formation of TiB₂ and AlN was established in samples sintered at temperatures above 1750 °C. The highest values of microhardness were found in samples sintered at the temperature range of 1850 – 2000 °C. Fracture toughness of samples practically does not change during thermobaric sintering Методом спекания при высоком давлении и высокой температуре изготовлен материал на основе кубического нитрида бора с использованием нитрида титана и алюминия в качестве связующей фазы. Объект исследования – структура, фазовый состав и физико-механические свойства материала. Установлено, что при температурах спекания выше 1750 °С в результате взаимодействия между компонентами шихты для спекания происходит образование диборида титана TiB₂ и AlN. Наивысшие значения микротвердости демонстрируют образцы, изготовленные в температурном интервале 1850–2000 °С. Трещиностойкость образцов практически не меняется в ходе термобарического спекания. Формирование структуры образцов происходит без укрупнения зерен композита, что свидетельствует об отсутствии собирательной рекристаллизации. Методом спікання при високому тиску і високій температурі виготовлено матеріал на основі кубічного нітриду бору з використанням нітриду титану та алюмінію як зв’язувальної фази. Об’єкт дослідження — структура, фазовий склад та фізико-механічні властивості матеріалу. Встановлено, що при температурах спікання вище 1750 °С в результаті взаємодії між компонентами шихти для спікання відбувається утворення дибориду титану TiB₂ та AlN. Найвищі значення мікротвердості демонструють зразки, виготовлені в температурному інтервалі 1850 – 2000 °С. Тріщиностійкість зразків практично не змінюється в ході термобаричного спікання. Формування структури зразків відбувається без укрупнення зерен композиту, що свідчить про відсутність збиральної рекристалізації. This research was supported by European Union’s Horizon 2020 Research and Innovation Programme under Flintstone2020 project (grant agreement No. 689279) and Visby Scholarship by the Swedish Institute (grant number02757/2016). en Інститут надтвердих матеріалів ім. В.М. Бакуля НАН України Породоразрушающий и металлообрабатывающий инструмент – техника и технология его изготовления и применения Инструментальные, конструкционные и функциональные материалы на основе алмаза и кубического нитрида бора cBN based materials with TiN-Al binder phase: sintering, structure, properties Матеріали на основі КНБ зі звязкою TiN-Al: спікання. структура, властивості Article published earlier |
| institution |
Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| collection |
DSpace DC |
| title |
cBN based materials with TiN-Al binder phase: sintering, structure, properties |
| spellingShingle |
cBN based materials with TiN-Al binder phase: sintering, structure, properties Slipchenko, K.V. Turkevich, V.Z. Bushlya, V.M. Ståhl, J.-E. Инструментальные, конструкционные и функциональные материалы на основе алмаза и кубического нитрида бора |
| title_short |
cBN based materials with TiN-Al binder phase: sintering, structure, properties |
| title_full |
cBN based materials with TiN-Al binder phase: sintering, structure, properties |
| title_fullStr |
cBN based materials with TiN-Al binder phase: sintering, structure, properties |
| title_full_unstemmed |
cBN based materials with TiN-Al binder phase: sintering, structure, properties |
| title_sort |
cbn based materials with tin-al binder phase: sintering, structure, properties |
| author |
Slipchenko, K.V. Turkevich, V.Z. Bushlya, V.M. Ståhl, J.-E. |
| author_facet |
Slipchenko, K.V. Turkevich, V.Z. Bushlya, V.M. Ståhl, J.-E. |
| topic |
Инструментальные, конструкционные и функциональные материалы на основе алмаза и кубического нитрида бора |
| topic_facet |
Инструментальные, конструкционные и функциональные материалы на основе алмаза и кубического нитрида бора |
| publishDate |
2019 |
| language |
English |
| container_title |
Породоразрушающий и металлообрабатывающий инструмент – техника и технология его изготовления и применения |
| publisher |
Інститут надтвердих матеріалів ім. В.М. Бакуля НАН України |
| format |
Article |
| title_alt |
Матеріали на основі КНБ зі звязкою TiN-Al: спікання. структура, властивості |
| description |
Cubic boron nitride material was produced via high pressure and high temperature sintering with titanium nitride and aluminum as binder phase. Microstructure, phase composition and physical-mechanical properties of the material were subject of current research. Formation of TiB₂ and AlN was established in samples sintered at temperatures above 1750 °C. The highest values of microhardness were found in samples sintered at the temperature range of 1850 – 2000 °C. Fracture toughness of samples practically does not change during thermobaric sintering
Методом спекания при высоком давлении и высокой температуре изготовлен материал на основе кубического нитрида бора с использованием нитрида титана и алюминия в качестве связующей фазы. Объект исследования – структура, фазовый состав и физико-механические свойства материала. Установлено, что при температурах спекания выше 1750 °С в результате взаимодействия между компонентами шихты для спекания происходит образование диборида титана TiB₂ и AlN. Наивысшие значения микротвердости демонстрируют образцы, изготовленные в температурном интервале 1850–2000 °С. Трещиностойкость образцов практически не меняется в ходе термобарического спекания. Формирование структуры образцов происходит без укрупнения зерен композита, что свидетельствует об отсутствии собирательной рекристаллизации.
Методом спікання при високому тиску і високій температурі виготовлено матеріал на основі кубічного нітриду бору з використанням нітриду титану та алюмінію як зв’язувальної фази. Об’єкт дослідження — структура, фазовий склад та фізико-механічні властивості матеріалу. Встановлено, що при температурах спікання вище 1750 °С в результаті взаємодії між компонентами шихти для спікання відбувається утворення дибориду титану TiB₂ та AlN. Найвищі значення мікротвердості демонструють зразки, виготовлені в температурному інтервалі 1850 – 2000 °С. Тріщиностійкість зразків практично не змінюється в ході термобаричного спікання. Формування структури зразків відбувається без укрупнення зерен композиту, що свідчить про відсутність збиральної рекристалізації.
|
| issn |
2223-3938 |
| url |
https://nasplib.isofts.kiev.ua/handle/123456789/159970 |
| citation_txt |
cBN based materials with TiN-Al binder phase: sintering, structure, properties / K.V. Slipchenko, V.Z. Turkevich, V.M. Bushlya, J.-E. Ståhl // Породоразрушающий и металлообрабатывающий инструмент – техника и технология его изготовления и применения: Сб. науч. тр. — К.: ІНМ ім. В.М. Бакуля НАН України, 2019. — Вип. 22. — С. 254-260. — Бібліогр.: 14 назв. — англ. |
| work_keys_str_mv |
AT slipchenkokv cbnbasedmaterialswithtinalbinderphasesinteringstructureproperties AT turkevichvz cbnbasedmaterialswithtinalbinderphasesinteringstructureproperties AT bushlyavm cbnbasedmaterialswithtinalbinderphasesinteringstructureproperties AT stahlje cbnbasedmaterialswithtinalbinderphasesinteringstructureproperties AT slipchenkokv materíalinaosnovíknbzízvâzkoûtinalspíkannâstrukturavlastivostí AT turkevichvz materíalinaosnovíknbzízvâzkoûtinalspíkannâstrukturavlastivostí AT bushlyavm materíalinaosnovíknbzízvâzkoûtinalspíkannâstrukturavlastivostí AT stahlje materíalinaosnovíknbzízvâzkoûtinalspíkannâstrukturavlastivostí |
| first_indexed |
2025-12-07T19:41:16Z |
| last_indexed |
2025-12-07T19:41:16Z |
| _version_ |
1850879746385117184 |