Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides
For WC–6 wt % Co and WC–6 wt % Ni composites, and by using five parameter analysis method as a new approach, the geometric and crystallographic features of carbide/carbide boundaries have been characterized. Two most frequently occurring WC/WC boundaries are 90° twist boundaries about [10-10] (Σ2 bo...
Gespeichert in:
| Veröffentlicht in: | Сверхтвердые материалы |
|---|---|
| Datum: | 2019 |
| 1. Verfasser: | |
| Format: | Artikel |
| Sprache: | English |
| Veröffentlicht: |
Інститут надтвердих матеріалів ім. В.М. Бакуля НАН України
2019
|
| Schlagworte: | |
| Online Zugang: | https://nasplib.isofts.kiev.ua/handle/123456789/167316 |
| Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
| Назва журналу: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| Zitieren: | Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides / Xiaokun Yuan // Надтверді матеріали. — 2019. — № 4 (240). — С. 23-32. — Бібліогр.: 12 назв. — англ. |
Institution
Digital Library of Periodicals of National Academy of Sciences of Ukraine| id |
nasplib_isofts_kiev_ua-123456789-167316 |
|---|---|
| record_format |
dspace |
| spelling |
Xiaokun Yuan 2020-03-25T09:53:44Z 2020-03-25T09:53:44Z 2019 Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides / Xiaokun Yuan // Надтверді матеріали. — 2019. — № 4 (240). — С. 23-32. — Бібліогр.: 12 назв. — англ. 0203-3119 https://nasplib.isofts.kiev.ua/handle/123456789/167316 669.275:539.27 For WC–6 wt % Co and WC–6 wt % Ni composites, and by using five parameter analysis method as a new approach, the geometric and crystallographic features of carbide/carbide boundaries have been characterized. Two most frequently occurring WC/WC boundaries are 90° twist boundaries about [10-10] (Σ2 boundaries) and 27.8° twist boundaries about [0001] (Σ13a boundaries), the Σ2 boundary populations vary with binder phase types, and carbide crystals are most frequently terminated by (0001) and (10-10) surfaces, such preference does not significantly alter if Σ2 boundaries are partitioned. Визначено геометричні і кристалографічні особливості на межі карбідно-карбідних переходів для композитів WC–6 % (за масою) Co і WC–6 % (за масою) методом аналізу п’яти параметрів. Дві межі WC/WC, що найчастіше зустрічаються, – це поворот межі на 90° приблизно [10-10] (межі Σ2) і поворот межі на 27,8° приблизно [0001] (межі Σ13a), сукупності межі Σ2 змінюються в залежності від типів сполучених фаз і кристалів карбіду і найчастіше закінчуються поверхнями (0001) і (10-10), така перевага суттєво не змінюється, якщо межі Σ2 розділені. Определены геометрические и кристаллографические особенности на границах карбидно-карбидных переходов для композитов WC–6% (по массе) Co и WC–6% (по массе) методом анализа пяти параметров. Наиболее часто встречающиеся две границы WC/WC – это поворот границ на 90°, приблизительно [10-10] (границы Σ2), и поворот границ на 27,8°, приблизительно [0001] (границы Σ13a), совокупности границ Σ2 меняются в зависимости от типов соединенных фаз и кристаллов карбида и чаще всего заканчиваются поверхностями (0001) и (10-10), такое предпочтение существенно не меняется, если границы Σ2 разделены. The author acknowledges support from National Natural Science Foundation of China (51471007). en Інститут надтвердих матеріалів ім. В.М. Бакуля НАН України Сверхтвердые материалы Одержання, структура, властивості Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides Article published earlier |
| institution |
Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| collection |
DSpace DC |
| title |
Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides |
| spellingShingle |
Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides Xiaokun Yuan Одержання, структура, властивості |
| title_short |
Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides |
| title_full |
Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides |
| title_fullStr |
Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides |
| title_full_unstemmed |
Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides |
| title_sort |
effect of different binder phases on the σ2 grain boundary plane distribution in cemented carbides |
| author |
Xiaokun Yuan |
| author_facet |
Xiaokun Yuan |
| topic |
Одержання, структура, властивості |
| topic_facet |
Одержання, структура, властивості |
| publishDate |
2019 |
| language |
English |
| container_title |
Сверхтвердые материалы |
| publisher |
Інститут надтвердих матеріалів ім. В.М. Бакуля НАН України |
| format |
Article |
| description |
For WC–6 wt % Co and WC–6 wt % Ni composites, and by using five parameter analysis method as a new approach, the geometric and crystallographic features of carbide/carbide boundaries have been characterized. Two most frequently occurring WC/WC boundaries are 90° twist boundaries about [10-10] (Σ2 boundaries) and 27.8° twist boundaries about [0001] (Σ13a boundaries), the Σ2 boundary populations vary with binder phase types, and carbide crystals are most frequently terminated by (0001) and (10-10) surfaces, such preference does not significantly alter if Σ2 boundaries are partitioned.
Визначено геометричні і кристалографічні особливості на межі карбідно-карбідних переходів для композитів WC–6 % (за масою) Co і WC–6 % (за масою) методом аналізу п’яти параметрів. Дві межі WC/WC, що найчастіше зустрічаються, – це поворот межі на 90° приблизно [10-10] (межі Σ2) і поворот межі на 27,8° приблизно [0001] (межі Σ13a), сукупності межі Σ2 змінюються в залежності від типів сполучених фаз і кристалів карбіду і найчастіше закінчуються поверхнями (0001) і (10-10), така перевага суттєво не змінюється, якщо межі Σ2 розділені.
Определены геометрические и кристаллографические особенности на границах карбидно-карбидных переходов для композитов WC–6% (по массе) Co и WC–6% (по массе) методом анализа пяти параметров. Наиболее часто встречающиеся две границы WC/WC – это поворот границ на 90°, приблизительно [10-10] (границы Σ2), и поворот границ на 27,8°, приблизительно [0001] (границы Σ13a), совокупности границ Σ2 меняются в зависимости от типов соединенных фаз и кристаллов карбида и чаще всего заканчиваются поверхностями (0001) и (10-10), такое предпочтение существенно не меняется, если границы Σ2 разделены.
|
| issn |
0203-3119 |
| url |
https://nasplib.isofts.kiev.ua/handle/123456789/167316 |
| citation_txt |
Effect of different binder phases on the Σ2 grain boundary plane distribution in cemented carbides / Xiaokun Yuan // Надтверді матеріали. — 2019. — № 4 (240). — С. 23-32. — Бібліогр.: 12 назв. — англ. |
| work_keys_str_mv |
AT xiaokunyuan effectofdifferentbinderphasesontheσ2grainboundaryplanedistributionincementedcarbides |
| first_indexed |
2025-12-02T11:03:02Z |
| last_indexed |
2025-12-02T11:03:02Z |
| _version_ |
1850862277775851520 |