Influence of H₂S Corrosion on Tensile Properties and Fracture Toughness of X80 Pipeline Steel
Tensile and fracture properties of X80 pipeline steel were studied in a mimic petrochemical environment. X80 pipeline steel specimens were firstly exposed to air or H₂S corrosive medium. Then their tensile properties and δ-Δa resistance curves were obtained in experiments. The influence of H₂S corro...
Saved in:
| Date: | 2019 |
|---|---|
| Main Authors: | Gu, L., Wang, J., Luan, C.B. |
| Format: | Article |
| Language: | English |
| Published: |
Інститут проблем міцності ім. Г.С. Писаренко НАН України
2019
|
| Series: | Проблемы прочности |
| Subjects: | |
| Online Access: | https://nasplib.isofts.kiev.ua/handle/123456789/188314 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Journal Title: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| Cite this: | Influence of H₂S Corrosion on Tensile Properties and Fracture Toughness of X80 Pipeline Steel / L. Gu, J. Wang, C.B. Luan, X.Y. Li // Проблеми міцності. — 2019. — № 1. — С. 163-174. — Бібліогр.: 22 назв. — англ. |
Institution
Digital Library of Periodicals of National Academy of Sciences of UkraineSimilar Items
-
Interfacial Fracture Toughness of Multilayer Composite Structures
by: Her, S.-C., et al.
Published: (2015) -
Fracture Toughness and Crack Resistance of Steam Pipeline Steel in Initial and Used States
by: Zrilic, M., et al.
Published: (2004) -
Fracture toughness of multilayer pipes
by: Nezbedova, E., et al.
Published: (2008) -
Tensile Fracture Analysis of Key-Hole Notches by Means of the Strain Energy Density
by: Torabi, A.R., et al.
Published: (2016) -
Experimental-Numerical Study of Tensile Strength of the High-Strength Steel S690QL at Elevated Temperatures
by: Arsić, D., et al.
Published: (2016)