Leaching of uranium ores in the process of sodium sulphate electrolysis

When uranium is extracted from concentrates with high silicon content, acid leaching is usually used. The disadvantage of this method is the high consumption, high cost and corrosion activity of the reagents. Moreover, for the oxidation of tetravalent uranium to highly soluble hexavalent uranium, it...

Full description

Saved in:
Bibliographic Details
Published in:Вопросы атомной науки и техники
Date:2019
Main Authors: Nefedov, V.G., Sknar, Yu.E., Kharytonova, O.A.
Format: Article
Language:English
Published: Національний науковий центр «Харківський фізико-технічний інститут» НАН України 2019
Subjects:
Online Access:https://nasplib.isofts.kiev.ua/handle/123456789/195228
Tags: Add Tag
No Tags, Be the first to tag this record!
Journal Title:Digital Library of Periodicals of National Academy of Sciences of Ukraine
Cite this:Leaching of uranium ores in the process of sodium sulphate electrolysis / V.G. Nefedov, Yu.E. Sknar, O.A. Kharytonova // Problems of atomic science and technology. — 2019. — № 5. — С. 113-117. — Бібліогр.: 2 назв. — англ.

Institution

Digital Library of Periodicals of National Academy of Sciences of Ukraine
_version_ 1862624431648538624
author Nefedov, V.G.
Sknar, Yu.E.
Kharytonova, O.A.
author_facet Nefedov, V.G.
Sknar, Yu.E.
Kharytonova, O.A.
citation_txt Leaching of uranium ores in the process of sodium sulphate electrolysis / V.G. Nefedov, Yu.E. Sknar, O.A. Kharytonova // Problems of atomic science and technology. — 2019. — № 5. — С. 113-117. — Бібліогр.: 2 назв. — англ.
collection DSpace DC
container_title Вопросы атомной науки и техники
description When uranium is extracted from concentrates with high silicon content, acid leaching is usually used. The disadvantage of this method is the high consumption, high cost and corrosion activity of the reagents. Moreover, for the oxidation of tetravalent uranium to highly soluble hexavalent uranium, it is necessary to process it with oxidizing agents, for example, oxygen. The work shows the possibility of development and chemical concentration of uranium ores using electrolysis of sodium sulfate. During electrolysis the pH in the anode chambers ranges from 2.2…2.5 to 0.5…0.7 in the near-electrode layer of the electrolyte, which corresponds to the pH range during leaching in agitators. Oxygen released at the anode is able to oxidize uranium to hexavalent one. Під час вилучення урану з концентратів з високим вмістом оксиду кремнію зазвичай застосовується кислотне вилуговування. Недоліками такого способу є велика витрата, висока вартість і корозійна активність реагентів. При цьому для окислення чотирьохвалентного урану до добре розчинного шестивалентного необхідна операція його обробки окислювачами, наприклад, киснем. У роботі показана можливість розтину і хімічного концентрування уранових руд за допомогою електролізу сульфату натрію. рН в анодних камерах при електролізі коливається від 2,2…2,5 до 0,5…0,7 в приелектродному шарі електроліту, що відповідає діапазону рН при вилуговуванні в агітаторах. Кисень, що виділяється на аноді, здатний окислювати уран до шестивалентного. При извлечении урана из концентратов с высоким содержанием оксида кремния обычно применяется кислотное выщелачивание. Недостатками такого способа являются большой расход, высокая стоимость и коррозионная активность реагентов. При этом для окисления четырехвалентного урана до хорошо растворимого шестивалентного необходима операция его обработки окислителями, например, кислородом. В работе показана возможность вскрытия и химического концентрирования урановых руд с помощью электролиза сульфата натрия. рН в анодных камерах при электролизе колеблется от 2,2…2,5 до 0,5…0,7 в приэлектродном слое электролита, что соответствует диапазону рН при выщелачивании в агитаторах. Выделяющийся на аноде кислород способен окислять уран до шестивалентного.
first_indexed 2025-12-07T13:31:52Z
format Article
fulltext
id nasplib_isofts_kiev_ua-123456789-195228
institution Digital Library of Periodicals of National Academy of Sciences of Ukraine
issn 1562-6016
language English
last_indexed 2025-12-07T13:31:52Z
publishDate 2019
publisher Національний науковий центр «Харківський фізико-технічний інститут» НАН України
record_format dspace
spelling Nefedov, V.G.
Sknar, Yu.E.
Kharytonova, O.A.
2023-12-03T15:37:38Z
2023-12-03T15:37:38Z
2019
Leaching of uranium ores in the process of sodium sulphate electrolysis / V.G. Nefedov, Yu.E. Sknar, O.A. Kharytonova // Problems of atomic science and technology. — 2019. — № 5. — С. 113-117. — Бібліогр.: 2 назв. — англ.
1562-6016
https://nasplib.isofts.kiev.ua/handle/123456789/195228
621.357.1:661.883.1; 541.135
When uranium is extracted from concentrates with high silicon content, acid leaching is usually used. The disadvantage of this method is the high consumption, high cost and corrosion activity of the reagents. Moreover, for the oxidation of tetravalent uranium to highly soluble hexavalent uranium, it is necessary to process it with oxidizing agents, for example, oxygen. The work shows the possibility of development and chemical concentration of uranium ores using electrolysis of sodium sulfate. During electrolysis the pH in the anode chambers ranges from 2.2…2.5 to 0.5…0.7 in the near-electrode layer of the electrolyte, which corresponds to the pH range during leaching in agitators. Oxygen released at the anode is able to oxidize uranium to hexavalent one.
Під час вилучення урану з концентратів з високим вмістом оксиду кремнію зазвичай застосовується кислотне вилуговування. Недоліками такого способу є велика витрата, висока вартість і корозійна активність реагентів. При цьому для окислення чотирьохвалентного урану до добре розчинного шестивалентного необхідна операція його обробки окислювачами, наприклад, киснем. У роботі показана можливість розтину і хімічного концентрування уранових руд за допомогою електролізу сульфату натрію. рН в анодних камерах при електролізі коливається від 2,2…2,5 до 0,5…0,7 в приелектродному шарі електроліту, що відповідає діапазону рН при вилуговуванні в агітаторах. Кисень, що виділяється на аноді, здатний окислювати уран до шестивалентного.
При извлечении урана из концентратов с высоким содержанием оксида кремния обычно применяется кислотное выщелачивание. Недостатками такого способа являются большой расход, высокая стоимость и коррозионная активность реагентов. При этом для окисления четырехвалентного урана до хорошо растворимого шестивалентного необходима операция его обработки окислителями, например, кислородом. В работе показана возможность вскрытия и химического концентрирования урановых руд с помощью электролиза сульфата натрия. рН в анодных камерах при электролизе колеблется от 2,2…2,5 до 0,5…0,7 в приэлектродном слое электролита, что соответствует диапазону рН при выщелачивании в агитаторах. Выделяющийся на аноде кислород способен окислять уран до шестивалентного.
en
Національний науковий центр «Харківський фізико-технічний інститут» НАН України
Вопросы атомной науки и техники
Thermal and fast reactor materials
Leaching of uranium ores in the process of sodium sulphate electrolysis
Розкриття уранових руд у процесі електролізу сульфату натрію
Вскрытие урановых руд в процессе электролиза сульфата натрия
Article
published earlier
spellingShingle Leaching of uranium ores in the process of sodium sulphate electrolysis
Nefedov, V.G.
Sknar, Yu.E.
Kharytonova, O.A.
Thermal and fast reactor materials
title Leaching of uranium ores in the process of sodium sulphate electrolysis
title_alt Розкриття уранових руд у процесі електролізу сульфату натрію
Вскрытие урановых руд в процессе электролиза сульфата натрия
title_full Leaching of uranium ores in the process of sodium sulphate electrolysis
title_fullStr Leaching of uranium ores in the process of sodium sulphate electrolysis
title_full_unstemmed Leaching of uranium ores in the process of sodium sulphate electrolysis
title_short Leaching of uranium ores in the process of sodium sulphate electrolysis
title_sort leaching of uranium ores in the process of sodium sulphate electrolysis
topic Thermal and fast reactor materials
topic_facet Thermal and fast reactor materials
url https://nasplib.isofts.kiev.ua/handle/123456789/195228
work_keys_str_mv AT nefedovvg leachingofuraniumoresintheprocessofsodiumsulphateelectrolysis
AT sknaryue leachingofuraniumoresintheprocessofsodiumsulphateelectrolysis
AT kharytonovaoa leachingofuraniumoresintheprocessofsodiumsulphateelectrolysis
AT nefedovvg rozkrittâuranovihruduprocesíelektrolízusulʹfatunatríû
AT sknaryue rozkrittâuranovihruduprocesíelektrolízusulʹfatunatríû
AT kharytonovaoa rozkrittâuranovihruduprocesíelektrolízusulʹfatunatríû
AT nefedovvg vskrytieuranovyhrudvprocesseélektrolizasulʹfatanatriâ
AT sknaryue vskrytieuranovyhrudvprocesseélektrolizasulʹfatanatriâ
AT kharytonovaoa vskrytieuranovyhrudvprocesseélektrolizasulʹfatanatriâ