The pyrocarbon, gas phase densification of the catalytic carbon formations (CCFs), obtained on iron
Investigations on gas-phase densification of CCFs, obtained on iron, using the radially driven pyrolysis zone and, at the same time, the temperature rise in the pyrolysis zone with the speed of the 1.25 °С/h, were carried out. CCFs, bonded with pyrocarbon (CCFBPyC), not refined from iron, without de...
Saved in:
| Published in: | Problems of Atomic Science and Technology |
|---|---|
| Date: | 2023 |
| Main Authors: | , , |
| Format: | Article |
| Language: | English |
| Published: |
Національний науковий центр «Харківський фізико-технічний інститут» НАН України
2023
|
| Subjects: | |
| Online Access: | https://nasplib.isofts.kiev.ua/handle/123456789/196113 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Journal Title: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
| Cite this: | The pyrocarbon, gas phase densification of the catalytic carbon formations (CCFs), obtained on iron / S.G. Fursov, M.V. Meltyukhov, S.A. Lyashenko // Problems of Atomic Science and Technology. — 2023. — № 2. — С. 153-156. — Бібліогр.: 7 назв. — англ. |
Institution
Digital Library of Periodicals of National Academy of Sciences of Ukraine| Summary: | Investigations on gas-phase densification of CCFs, obtained on iron, using the radially driven pyrolysis zone and, at the same time, the temperature rise in the pyrolysis zone with the speed of the 1.25 °С/h, were carried out. CCFs, bonded with pyrocarbon (CCFBPyC), not refined from iron, without defects, with density and PyC content corresponding to the material: graphite bonded with pyrocarbon (GBPyC), which include 90 wt.% of PyC (GBPyC-90), were obtained. The necessity of applying the special technological methods in the process of gas-phase densification of CCFs, was confirmed.
Досліджене газофазне ущільнення піровуглецем каталітичних утворень вуглецю (КУВ) на Fe за допомогою методу зони піролізу, що радіально рухається, з одночасним підвищенням температури в зоні піролізу зі швидкістю 1,25 ° С/год. Отримані бездефектні КУВ зв’язані піровуглецем (КУВЗП) з невидаленим каталізатором, зі щільністю і вмістом піровуглецю на рівні матеріалу: графіт, з’язаний піровуглецем, з його вмістом – 90 ваг.% (ГЗП-90). Підтверджена необхідність застосування спеціальних технологічних прийомів при ущільненні піровуглецем КУВ.
|
|---|---|
| ISSN: | 1562-6016 |