The paper presents the results of a study of the physical and chemical properties of narrow fractions of diamond nanopowders with a low content of non-diamond carbon grade ASUD-99. Six fractions with different average diameters of diamond particle aggregates from 28.785 to 3.891 μm were obtained by...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Datum:2020
Hauptverfasser: Ільницька, Г. Д., Логінова, О. Б., Смоквина, В. В., Зайцева, І. М., Довга, О. В.
Format: Artikel
Sprache:Englisch
Veröffentlicht: Chuiko Institute of Surface Chemistry National Academy of Sciences of Ukraine 2020
Schlagworte:
Online Zugang:https://surfacezbir.com.ua/index.php/surface/article/view/707
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Назва журналу:Surface
Завантажити файл: Pdf

Institution

Surface
Beschreibung
Zusammenfassung:The paper presents the results of a study of the physical and chemical properties of narrow fractions of diamond nanopowders with a low content of non-diamond carbon grade ASUD-99. Six fractions with different average diameters of diamond particle aggregates from 28.785 to 3.891 μm were obtained by separating a 0.2 % aqueous suspension of the initial powders by the sedimentation method. It has been found that the smallest aggregates consist of larger particles with a smaller specific surface area and a lower interaction energy between them. This conclusion is confirmed by a decrease in the porosity of the obtained aggregates. So, if the pore volume in the largest aggregates of diamond particles is 0.859 ml/g, then in the smallest 0.550 ml/g, while the pore radius of diamond aggregates in different fractions changes insignificantly. Separation in a magnetic field at different currents of diamond nanopowders with a specific magnetic susceptibility of 0.52×10-8 m3 kg, treated with a solution of 5 % iron chloride, made it possible to obtain five fractions that differ from each other in specific magnetic susceptibility (c) – from magnetic fractions with c = 4.30×10-8 m3/kg to diamagnetic – with c = –0.11×10-8 m3/kg. It is shown that the modification of diamond nanopowders with iron ions increases the separation selectivity and makes it possible to isolate diamagnetic powders.