РОЗПОДІЛЕННЯ ЧАСТИНОК ЗА РОЗМІРАМИ ТА МАГНІТНІ ХАРАКТЕРИСТИКИ ШЛАМУ, ЯКИЙ ОТРИМУЮТЬ ПРИ ОБРОБЦІ ПІСКОВИКУ ФУНКЦІОНАЛЬНИМИ ЕЛЕМЕНТАМИ З КАМ НА МЕТАЛЕВИХ ЗВ´ЯЗКАХ

The results of a study of the sludge of sandstone treatment of the Torez field t with experimental CDM (composite diamond materials) functional elements based on the bunch  material Ni(94%)-Sn(6%), equipped with diamond inclusions. CDM are made by the method of intense sintering under a pre...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Datum:2020
Hauptverfasser: Васильчук, О.С., Майстренко, А.Л., Петасюк , Г.А., Олійник, Н.А., Ільницька, Г.Д., Віноградова, О.П., Закора, А.П., Базалій, Г.А.
Format: Artikel
Sprache:Ukrainian
Veröffentlicht: Институт сверхтвердых материалов им. В. Н. Бакуля Национальной академии наук Украины 2020
Schlagworte:
Online Zugang:http://altis-ism.org.ua/index.php/ALTIS/article/view/157
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Назва журналу:Tooling materials science

Institution

Tooling materials science
Beschreibung
Zusammenfassung:The results of a study of the sludge of sandstone treatment of the Torez field t with experimental CDM (composite diamond materials) functional elements based on the bunch  material Ni(94%)-Sn(6%), equipped with diamond inclusions. CDM are made by the method of intense sintering under a pressure 300 MPa are presented. It was found that the particle size and the size distribution interval of the sludge particles that were installed using the DiaInspect.OSM device from VOLLSTÄDT DIАMANT GmbH decrease with increasing intensity wear from 75 to 170 mg / km. More than 90% of the amount of sludge particles is distributed in the range of sizes12-90 microns. The specific magnetic susceptibility of the components of the sludge is equal to: sandstone of the Torez field - 2.36∙10-8 m3/kg, diamond powder grade AC 200 with a grain size of 400/315 - 8.4∙10-8 m3/kg, metal-containing components of CDM functional elements - (9000-10000)∙10-8 m3/kg. The specific magnetic susceptibility depends on the intensity wear of the functional elements with CDM. An increase of the intensity wear of functional elements from 75 to 170 mg/km leads to an increase in the specific magnetic susceptibility of the sludge to 2 times, a magnetic fraction to 1.5 times, and a content of the magnetic fraction to 1.8 times.