Особливості виникнення стартових віял при безперервному розливанні сортової заготівки відкритим струменем: Processy litʹâ, 2019, Tom 133, №1, p.23-30

Reсeived 05.11.2018 UDK 669.74.047 The specificity of casting billet on multi-varietal continuous caster is the inability to control the quality of each billet, including their surface. This paper presents the results of industrial studies of the conditions for the occurrence of surface defects asso...

Full description

Saved in:
Bibliographic Details
Date:2019
Main Authors: Смірнов, О. М., Рябий, Д. В., Верзілов, О. П.
Format: Article
Language:Ukrainian
Published: National Academy of Sciences of Ukraine, Physical-Technological Institute of Metals and Alloys of NAS of Ukraine 2019
Subjects:
Online Access:https://plit-periodical.org.ua/index.php/plit/article/view/149
Tags: Add Tag
No Tags, Be the first to tag this record!
Journal Title:Casting Processes

Institution

Casting Processes
Description
Summary:Reсeived 05.11.2018 UDK 669.74.047 The specificity of casting billet on multi-varietal continuous caster is the inability to control the quality of each billet, including their surface. This paper presents the results of industrial studies of the conditions for the occurrence of surface defects associated with spraying of steel at the site of the industrial-bucket batcher and the mold of the sectional caster, as well as an assessment of the possibility of reducing the phenomenon of rhenium during the start of the caster. This publication also presents the results of apply-ing «gauge» inserts for dosing glasses with alternative chemical composition. The results of the work tes-tify to the prospect of research aimed at the use of «gauge» dosing glasses with alternative chemical composition, allowing for a stable outflow of the metal jet at the start of the continuous casting machine series.