Про ядерне гідрування оболонок твелів з цирконію та його сплавів у реакторі типу ВВЕР-1000
The paper considers physical models of nuclear hydrogenation of fuel claddings made of zirconium and its alloys that occurs in neutron fields of the WWER cores with uranium dioxide fuel. This causes the cladding material to lose its plasticity and leads to cracks during operation.
Saved in:
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | Ukrainian |
Published: |
State Scientific and Technical Center for Nuclear and Radiation Safety
2013
|
Online Access: | https://nuclear-journal.com/index.php/journal/article/view/483 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|