Properties of 13KhMF steel after operation and degradation in laboratory conditions
Saved in:
| Date: | 2010 |
|---|---|
| Main Author: | I. R. Dzioba |
| Format: | Article |
| Language: | English |
| Published: |
2010
|
| Series: | Materials Science (Physicochemical mechanics of materials) |
| Online Access: | http://jnas.nbuv.gov.ua/article/UJRN-0000657125 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Journal Title: | Library portal of National Academy of Sciences of Ukraine | LibNAS |
Institution
Library portal of National Academy of Sciences of Ukraine | LibNASSimilar Items
The influence of microstructure components on static crack growth resistance of 13KhMF steel
by: I. R. Dzioba
Published: (2011)
by: I. R. Dzioba
Published: (2011)
Computer analysis of surface morphology of 15Kh13MF steel after laser pulse treatment
by: P. O. Marushchak, et al.
Published: (2013)
by: P. O. Marushchak, et al.
Published: (2013)
Operation degradation of 20Kh13 steel blades of HPP steam turbines
by: H. M. Nykyforchyn, et al.
Published: (2011)
by: H. M. Nykyforchyn, et al.
Published: (2011)
Automatic selection and quantitative analysis of carbides on the 12Kh1MF steel grains interface after operation at the HPP pipeline
by: R. A. Vorobel, et al.
Published: (2011)
by: R. A. Vorobel, et al.
Published: (2011)
Method of laboratory degradation of structural steels
by: O. T. Tsyrulnyk, et al.
Published: (2017)
by: O. T. Tsyrulnyk, et al.
Published: (2017)
Modeling of service degradation of steels of cargo port constructions in laboratory conditions
by: V. M. Pustovoi, et al.
Published: (2012)
by: V. M. Pustovoi, et al.
Published: (2012)
Peculiarities of fine structure and local stress state of 13Kh11N2V2MF steel under cyclic loading
by: Z. A. Duriahina, et al.
Published: (2021)
by: Z. A. Duriahina, et al.
Published: (2021)
Computer assessing the variation of grain size of the exploited 12Kh1MF steel structure
by: I. M. Zhuravel
Published: (2019)
by: I. M. Zhuravel
Published: (2019)
Anisotropy of the mechanical properties of 15Kh1M1F degraded steel after its exploitation on HPP pipelines
by: O. Z. Student, et al.
Published: (2011)
by: O. Z. Student, et al.
Published: (2011)
Features of structure formation of surface layers with high content of boron on steel 15Kh11MF in the conditions of furnace and induction heating
by: S. A. Kniaziev
Published: (2020)
by: S. A. Kniaziev
Published: (2020)
Influence of low-temperature tempered structure and properties of welded joints of high-strength steel 30Kh2N2MF
by: O. A. Haivoronskyi, et al.
Published: (2020)
by: O. A. Haivoronskyi, et al.
Published: (2020)
Develop¬ment of in-laboratory method of steel degradation for assessing their crack growth resistance
by: M. I. Hredil, et al.
Published: (2021)
by: M. I. Hredil, et al.
Published: (2021)
Operational degradation of structural steels (A review)
by: O. I. Zvirko
Published: (2021)
by: O. I. Zvirko
Published: (2021)
Influence of 17HIS steel degradation on its properties after service on the main pipeline
by: Ye. V. Kharchenko, et al.
Published: (2017)
by: Ye. V. Kharchenko, et al.
Published: (2017)
Effect of thermal cycle of welding on structural-phase transformations and properties of HAZ metal of medium-carbon alloyed steel of 30Kh2N2MF type
by: V. D. Poznjakov, et al.
Published: (2015)
by: V. D. Poznjakov, et al.
Published: (2015)
Diagnostics of pipe steel susceptibility to property degradation as a result of long-term operation
by: H. M. Nykyforchyn, et al.
Published: (2016)
by: H. M. Nykyforchyn, et al.
Published: (2016)
Use of electrochemical methods for evaluation of operational degradation of structural steels
by: O. I. Zvirko
Published: (2016)
by: O. I. Zvirko
Published: (2016)
Heat treatment influence on the steel 15X11MF wear resistance
by: M. A. Pohribnyi, et al.
Published: (2014)
by: M. A. Pohribnyi, et al.
Published: (2014)
Titans of Ukraine. UPTI–laboratory No. 1–KhPTI
by: A. Tanshyna
Published: (2019)
by: A. Tanshyna
Published: (2019)
Titans of Ukraine. UPTI–laboratory No. 1–KhPTI
by: A. Tanshyna
Published: (2019)
by: A. Tanshyna
Published: (2019)
The evaluation of operational degradation of gas pipeline steels by the mechanical stability criterion
by: Yu. Ya. Mieshkov, et al.
Published: (2014)
by: Yu. Ya. Mieshkov, et al.
Published: (2014)
Ranking of mechanical characteristics of HPP pipeline steels by their sensitivity to operational degradation
by: O. Z. Student, et al.
Published: (2021)
by: O. Z. Student, et al.
Published: (2021)
Electrochemical methods of evaluation of degradation of long-term operation structural steels
by: O. I. Zvirko
Published: (2016)
by: O. I. Zvirko
Published: (2016)
Degradation of 09H2S steel in the conditions of oil-refining
by: O. H. Arkhypov, et al.
Published: (2010)
by: O. H. Arkhypov, et al.
Published: (2010)
The influence of higher temperatures on mechanical characteristics of 26H2MF and St12T steels
by: V. Dudda
Published: (2019)
by: V. Dudda
Published: (2019)
Corrosion resistance of reinforced layers of 15Х11MF steel steam turbine blades
by: Hlushkova, D.B., et al.
Published: (2021)
by: Hlushkova, D.B., et al.
Published: (2021)
The influence of thermal cycles work on degradation of heat-resistant steel properties
by: P. O. Marushchak, et al.
Published: (2010)
by: P. O. Marushchak, et al.
Published: (2010)
Physicochemical properties of 40Kh carbonitrided steel
by: M. S. Stechyshyn, et al.
Published: (2020)
by: M. S. Stechyshyn, et al.
Published: (2020)
Physicochemical properties of carbonitrided KhVH steel
by: M. S. Stechyshyn, et al.
Published: (2020)
by: M. S. Stechyshyn, et al.
Published: (2020)
Degradation of structure and properties of metal of rails at the long-term operation
by: V. E. Gromov, et al.
Published: (2016)
by: V. E. Gromov, et al.
Published: (2016)
Fatigue life of specimens from 40KH steel after wear-resistant
by: V. V. Knysh, et al.
Published: (2021)
by: V. V. Knysh, et al.
Published: (2021)
Properties of steels of X13 type, alloyed with nitrogen
by: G. M. Grigorenko, et al.
Published: (2010)
by: G. M. Grigorenko, et al.
Published: (2010)
Research of operating characteristics of AVKM insertions at boring of granit plastins in laboratory conditions
by: Ju. V. Najdich, et al.
Published: (2016)
by: Ju. V. Najdich, et al.
Published: (2016)
The researches of high-temperature properties of iron materials in laboratory conditions
by: A. S. Nesterov, et al.
Published: (2018)
by: A. S. Nesterov, et al.
Published: (2018)
Restoration of heat-resistant steel properties after long-term operation in a steam pipeline
by: O. Z. Student, et al.
Published: (2021)
by: O. Z. Student, et al.
Published: (2021)
Service properties of 09G2S, 14KHGS steels and Steel 20 after long-term operation
by: S. A. Nedosieka, et al.
Published: (2020)
by: S. A. Nedosieka, et al.
Published: (2020)
Wear resistance of 30KhHSA steel in the conditions of rolling with slipping
by: O. O. Mikosianchyk, et al.
Published: (2019)
by: O. O. Mikosianchyk, et al.
Published: (2019)
Degradation of steel of excessively used reloading equipment
by: V. M. Pustovyi, et al.
Published: (2021)
by: V. M. Pustovyi, et al.
Published: (2021)
In-service degradation of pipe steel of grounding anodes
by: O. H. Arkhypov, et al.
Published: (2016)
by: O. H. Arkhypov, et al.
Published: (2016)
Molecular genetic identification of yeast isolate MF22_1
by: M. O. Fomina, et al.
Published: (2022)
by: M. O. Fomina, et al.
Published: (2022)
Similar Items
-
The influence of microstructure components on static crack growth resistance of 13KhMF steel
by: I. R. Dzioba
Published: (2011) -
Computer analysis of surface morphology of 15Kh13MF steel after laser pulse treatment
by: P. O. Marushchak, et al.
Published: (2013) -
Operation degradation of 20Kh13 steel blades of HPP steam turbines
by: H. M. Nykyforchyn, et al.
Published: (2011) -
Automatic selection and quantitative analysis of carbides on the 12Kh1MF steel grains interface after operation at the HPP pipeline
by: R. A. Vorobel, et al.
Published: (2011) -
Method of laboratory degradation of structural steels
by: O. T. Tsyrulnyk, et al.
Published: (2017)