Voievodin, V. M., Mytrofanov, A. S., Hozhenko, S. V., Vasylenko, R. L., Krainiuk, Y. O., Bazhukov, A. V., . . . Melnyk, Y. (2019). Non-metallic inclusions in 08Kh18N10T steel as a cause of defects in the heat exchange tubes of NPP steam generators.

Chicago-Zitierstil (17. Ausg.)

Voievodin, V. M., A. S. Mytrofanov, S. V. Hozhenko, R. L. Vasylenko, Ye. O. Krainiuk, A. V. Bazhukov, A. M. Palii, und Ye Melnyk. Non-metallic Inclusions in 08Kh18N10T Steel as a Cause of Defects in the Heat Exchange Tubes of NPP Steam Generators. 2019.

MLA-Zitierstil (8. Ausg.)

Voievodin, V. M., et al. Non-metallic Inclusions in 08Kh18N10T Steel as a Cause of Defects in the Heat Exchange Tubes of NPP Steam Generators. 2019.