Strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 K
Збережено в:
Дата: | 2011 |
---|---|
Автори: | , , , , , , , , |
Формат: | Стаття |
Мова: | English |
Опубліковано: |
2011
|
Назва видання: | Low Temperature Physics |
Онлайн доступ: | http://jnas.nbuv.gov.ua/article/UJRN-0000543373 |
Теги: |
Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
|
Назва журналу: | Library portal of National Academy of Sciences of Ukraine | LibNAS |
Репозитарії
Library portal of National Academy of Sciences of Ukraine | LibNASid |
open-sciencenbuvgovua-97740 |
---|---|
record_format |
dspace |
spelling |
open-sciencenbuvgovua-977402024-04-17T17:37:09Z Strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 K A. V. Podolskij S. N. Smirnov E. D. Tabachnikova V. Z. Bengus A. N. Velikodnyj M. A. Tikhonovskij B. Bonarski C. Mangler M. J. Zehetbauer 0132-6414 2011 en Low Temperature Physics http://jnas.nbuv.gov.ua/article/UJRN-0000543373 Article |
institution |
Library portal of National Academy of Sciences of Ukraine | LibNAS |
collection |
Open-Science |
language |
English |
series |
Low Temperature Physics |
spellingShingle |
Low Temperature Physics A. V. Podolskij S. N. Smirnov E. D. Tabachnikova V. Z. Bengus A. N. Velikodnyj M. A. Tikhonovskij B. Bonarski C. Mangler M. J. Zehetbauer Strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 K |
format |
Article |
author |
A. V. Podolskij S. N. Smirnov E. D. Tabachnikova V. Z. Bengus A. N. Velikodnyj M. A. Tikhonovskij B. Bonarski C. Mangler M. J. Zehetbauer |
author_facet |
A. V. Podolskij S. N. Smirnov E. D. Tabachnikova V. Z. Bengus A. N. Velikodnyj M. A. Tikhonovskij B. Bonarski C. Mangler M. J. Zehetbauer |
author_sort |
A. V. Podolskij |
title |
Strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 K |
title_short |
Strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 K |
title_full |
Strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 K |
title_fullStr |
Strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 K |
title_full_unstemmed |
Strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 K |
title_sort |
strain hardening and microstructure evolution during uniaxial compression of ultrafine grained zirconium in temperature range 4.2–300 k |
publishDate |
2011 |
url |
http://jnas.nbuv.gov.ua/article/UJRN-0000543373 |
work_keys_str_mv |
AT avpodolskij strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k AT snsmirnov strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k AT edtabachnikova strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k AT vzbengus strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k AT anvelikodnyj strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k AT matikhonovskij strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k AT bbonarski strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k AT cmangler strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k AT mjzehetbauer strainhardeningandmicrostructureevolutionduringuniaxialcompressionofultrafinegrainedzirconiumintemperaturerange42300k |
first_indexed |
2024-04-18T05:31:09Z |
last_indexed |
2024-04-18T05:31:09Z |
_version_ |
1796887478865494016 |