Features of temperature-dependent internal friction at phase decomposition of Nb-Ti alloy
Experimental dependence of internal friction Q⁻¹(T) on heating temperature T of pre-strained Nb-(48.5±1,5)Ti (wt. %) alloy is a superposition of two internal friction peaks with maxima at 250°C and 300°C. It is shown by calculation that both the peaks are due to nucleation and subsequent diffusion-c...
Saved in:
Main Author: | |
---|---|
Format: | Article |
Language: | English |
Published: |
НТК «Інститут монокристалів» НАН України
2008
|
Series: | Functional Materials |
Subjects: | |
Online Access: | http://dspace.nbuv.gov.ua/handle/123456789/135261 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|