Hydrogen Sorption Properties of Ti₀,₄₇₅Zr₀,₃Mn₀,₂₂₅ Eutectic Alloy Alloyed with 2 at.% and 5 at.% of Vanadium

Sorption properties and kinetic parameters of hydrogenating and dehydrogenating processes of Ti₀,₄₇₅Zr₀,₃Mn₀,₂₂₅ eutectic alloy, in which partial substitution of each of its component with 2% and 5% of vanadium is performed, are investigated by Sieverts’ method. As determined, the introduction of va...

Повний опис

Збережено в:
Бібліографічні деталі
Дата:2015
Автори: Ivanchenko, V.G., Dekhtyarenko, V.A., Pryadko, T.V.
Формат: Стаття
Мова:English
Опубліковано: Інститут металофізики ім. Г.В. Курдюмова НАН України 2015
Назва видання:Металлофизика и новейшие технологии
Теми:
Онлайн доступ:https://nasplib.isofts.kiev.ua/handle/123456789/111891
Теги: Додати тег
Немає тегів, Будьте першим, хто поставить тег для цього запису!
Назва журналу:Digital Library of Periodicals of National Academy of Sciences of Ukraine
Цитувати:Hydrogen Sorption Properties of Ti₀,₄₇₅Zr₀,₃Mn₀,₂₂₅ Eutectic Alloy Alloyed with 2 at.% and 5 at.% of Vanadium / V. G. Ivanchenko, V. A. Dekhtyarenko, T. V. Pryadko // Металлофизика и новейшие технологии. — 2015. — Т. 37, № 4. — С. 521-530. — Бібліогр.: 16 назв. — рос.

Репозитарії

Digital Library of Periodicals of National Academy of Sciences of Ukraine
Опис
Резюме:Sorption properties and kinetic parameters of hydrogenating and dehydrogenating processes of Ti₀,₄₇₅Zr₀,₃Mn₀,₂₂₅ eutectic alloy, in which partial substitution of each of its component with 2% and 5% of vanadium is performed, are investigated by Sieverts’ method. As determined, the introduction of vanadium within the specified limits results in decrease of the temperature of the start of intensive hydrogen absorption, decrease of the duration of hydrogenating process, and also in substantial increase of sorption capacity (up to 2.85% wt.). As shown, the alloys, which are subjected to the sorption—desorption cycling, possess as much activated surface that behave themselves with regard to hydrogen similar to intermetallic compounds and can absorb hydrogen at the room temperature and the pressure of 0.23 MPa from the first seconds of the contact of the specimen with the hydrogen-containing medium with the average rate of (2—4)∙10³ wt.%/s.