Diagnostics of hydrogen macrodelamination in the wall of pipe elbow of a natural gas transmission pipeline
Saved in:
| Date: | 2015 |
|---|---|
| Main Authors: | Ye. Kharchenko, Ye. Kunta, O. I. Zvirko, R. S. Savula, Z. A. Duriahina |
| Format: | Article |
| Language: | English |
| Published: |
2015
|
| Series: | Materials Science (Physicochemical mechanics of materials) |
| Online Access: | http://jnas.nbuv.gov.ua/article/UJRN-0000664248 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Journal Title: | Library portal of National Academy of Sciences of Ukraine | LibNAS |
Institution
Library portal of National Academy of Sciences of Ukraine | LibNASSimilar Items
Corrosion degradation of long-term operated gas pipeline elbow with macrodefect
by: O. I. Zvirko, et al.
Published: (2016)
by: O. I. Zvirko, et al.
Published: (2016)
Development of the method for assessment of serviceability and residual life of the main pipelines with service macrodelamination
by: O. T. Tsyrulnyk, et al.
Published: (2020)
by: O. T. Tsyrulnyk, et al.
Published: (2020)
The influence of hydrogenation of oil-and-gas pipeline walls on their soil corrosion and life
by: O. V. Hembara, et al.
Published: (2011)
by: O. V. Hembara, et al.
Published: (2011)
Procedure of ranging corrosion defects of the main gas pipelines found at in-pipe diagnostics
by: V. I. Makhnenko, et al.
Published: (2009)
by: V. I. Makhnenko, et al.
Published: (2009)
The influence of hydrogen on residual life of a gas pipeline pipe under manoeuvreing operation mode
by: Ye. Andreikiv, et al.
Published: (2015)
by: Ye. Andreikiv, et al.
Published: (2015)
Corrosion of an internal wall of industrial gas pipeline
by: Yu. Kovalenko, et al.
Published: (2012)
by: Yu. Kovalenko, et al.
Published: (2012)
The influence of gas pipeline long-term operation on fatigue crack growth resistance of 17H1S steel
by: Ye. V. Kharchenko, et al.
Published: (2016)
by: Ye. V. Kharchenko, et al.
Published: (2016)
Numerical analysis of the regularities of the infuence of pipe steel degradation on the reliability of corroded main gas pipelines used for transportation of gas-hydrogen mixtures
by: O. S. Milenin, et al.
Published: (2024)
by: O. S. Milenin, et al.
Published: (2024)
ropagation of a surface crack in the wall of an oil pipe, allowing for its hydrogenation
by: D. V. Rudavskyi
Published: (2012)
by: D. V. Rudavskyi
Published: (2012)
Peculiarities of corrosion-hydrogen degradation of oil and gas pipelines and oil tanks
by: Ye. I. Kryzhanivskyi, et al.
Published: (2011)
by: Ye. I. Kryzhanivskyi, et al.
Published: (2011)
On-line diagnostics of equipment in main gas pipelines systems Language: Russian
by: Linetsky I.K., et al.
Published: (2001)
by: Linetsky I.K., et al.
Published: (2001)
Crack initiation on pipeline inner surface in high-temperature service. Information 2. Stresses in pipe walls
by: S. A. Nedoseka, et al.
Published: (2015)
by: S. A. Nedoseka, et al.
Published: (2015)
The influence of the structural-mechanical state of the transit gas pipeline steel on the susceptibility to hydrogen embrittlement
by: O. I. Zvirko, et al.
Published: (2024)
by: O. I. Zvirko, et al.
Published: (2024)
Problems and prospects of transporting a mixture of green hydrogen and natural gas in the context of the development of hydrogen energy in Ukraine
by: O. I. Zvirko
Published: (2024)
by: O. I. Zvirko
Published: (2024)
Crack initiation on inner surface of pipelines at high temperatures. Information 3. Temperature and stresses in pipe wall at cooling
by: Ja. Nedoseka, et al.
Published: (2016)
by: Ja. Nedoseka, et al.
Published: (2016)
Estimation of stresses caused by electrochemical hydrogenation of pipe carbon steel
by: O. I. Zvirko, et al.
Published: (2024)
by: O. I. Zvirko, et al.
Published: (2024)
Diagnostics of hydrogen-oxygen plasma jet for application in gas thermal spraying
by: Yu. S. Popil, et al.
Published: (2020)
by: Yu. S. Popil, et al.
Published: (2020)
Unified Solutions on Plastic Limit Internal Pressure for Metallic Elbows
by: Zhu, Q, et al.
Published: (2014)
by: Zhu, Q, et al.
Published: (2014)
Unified Solutions on Plastic Limit Internal Pressure for Metallic Elbows
by: Q. Zhu, et al.
Published: (2014)
by: Q. Zhu, et al.
Published: (2014)
Diagnostics of pipe steel susceptibility to property degradation as a result of long-term operation
by: H. M. Nykyforchyn, et al.
Published: (2016)
by: H. M. Nykyforchyn, et al.
Published: (2016)
Implications of New Standards on Technical Diagnostics and Control Implementation for the Gas Transmission System Efficiency
by: Karpash, M.O., et al.
Published: (2019)
by: Karpash, M.O., et al.
Published: (2019)
Implications of New Standards on Technical Diagnostics and Control Implementation for the Gas Transmission System Efficiency
by: M. O. Karpash, et al.
Published: (2019)
by: M. O. Karpash, et al.
Published: (2019)
Calculation of large polyethylene pipes with a hollow wall
by: M. H. Stashchuk, et al.
Published: (2012)
by: M. H. Stashchuk, et al.
Published: (2012)
Off-line programs for operating diagnostics of main gas pipelines compressor stations equipment
by: Linetsky I.K., et al.
Published: (2001)
by: Linetsky I.K., et al.
Published: (2001)
Numerical assessment of brittle strength of field welds of the main gas pipelines at transportation of gas-hydrogen mixtures
by: O. S. Milenin, et al.
Published: (2023)
by: O. S. Milenin, et al.
Published: (2023)
The evaluation of operational degradation of gas pipeline steels by the mechanical stability criterion
by: Yu. Ya. Mieshkov, et al.
Published: (2014)
by: Yu. Ya. Mieshkov, et al.
Published: (2014)
Diagnostics and technique for the analysis pipelines transportation
by: Makharadze, L., et al.
Published: (2012)
by: Makharadze, L., et al.
Published: (2012)
Effect of localplastic deformations on physicomechanical properties of material and the pipeline stress state
by: Ye. V. Kharchenko, et al.
Published: (2013)
by: Ye. V. Kharchenko, et al.
Published: (2013)
The influence of the operated gas pipeline steels texture on their resistance to brittle fracture
by: O. I. Zvirko, et al.
Published: (2018)
by: O. I. Zvirko, et al.
Published: (2018)
Degradation of welded joint metal of the exploited main gas pipeline
by: O. T. Tsyrulnyk, et al.
Published: (2010)
by: O. T. Tsyrulnyk, et al.
Published: (2010)
Research of natural gas balance error in main gas pipelines system
by: Ильченко, Б. С., et al.
Published: (2016)
by: Ильченко, Б. С., et al.
Published: (2016)
Research of natural gas balance error in main gas pipelines system
by: Ильченко, Б. С., et al.
Published: (2016)
by: Ильченко, Б. С., et al.
Published: (2016)
Research of natural gas balance error in main gas pipelines system
by: B. S. Ilchenko, et al.
Published: (2010)
by: B. S. Ilchenko, et al.
Published: (2010)
Experimental and analytical evaluation of pipe steels hydrogenation
by: A. M. Syrotiuk, et al.
Published: (2017)
by: A. M. Syrotiuk, et al.
Published: (2017)
Methods for assessing corrosion hydrogen degradation of oil-gas piplenes steels
by: O. I. Zvirko, et al.
Published: (2020)
by: O. I. Zvirko, et al.
Published: (2020)
Increase of reliability of main pipelines by repeated flaw detection inside the pipes
by: D. P. Varlamov, et al.
Published: (2012)
by: D. P. Varlamov, et al.
Published: (2012)
RESEARCH INTO METHODS OF PIPE END DEMAGNETIZATION UNDER MAIN PIPELINE REPAIR
by: Dobrodeyev, P. N.
Published: (2014)
by: Dobrodeyev, P. N.
Published: (2014)
Equipment for preparation of pipe ends to welding of position butt joints of pipeline
by: L. M. Lobanov, et al.
Published: (2015)
by: L. M. Lobanov, et al.
Published: (2015)
To the question evacuation of natural gas from imperfect areas of diversion gas pipelines
by: Z. M. Matsuk, et al.
Published: (2016)
by: Z. M. Matsuk, et al.
Published: (2016)
Evaluation of residual life time of hydrogenated pipe by the acoustic signal parameters
by: V. R. Skalskyi, et al.
Published: (2015)
by: V. R. Skalskyi, et al.
Published: (2015)
Similar Items
-
Corrosion degradation of long-term operated gas pipeline elbow with macrodefect
by: O. I. Zvirko, et al.
Published: (2016) -
Development of the method for assessment of serviceability and residual life of the main pipelines with service macrodelamination
by: O. T. Tsyrulnyk, et al.
Published: (2020) -
The influence of hydrogenation of oil-and-gas pipeline walls on their soil corrosion and life
by: O. V. Hembara, et al.
Published: (2011) -
Procedure of ranging corrosion defects of the main gas pipelines found at in-pipe diagnostics
by: V. I. Makhnenko, et al.
Published: (2009) -
The influence of hydrogen on residual life of a gas pipeline pipe under manoeuvreing operation mode
by: Ye. Andreikiv, et al.
Published: (2015)